Several chemical reactions are able to produce swelling of concrete for decades after its initial curing, a problem that affects a considerable number of concrete dams around the world. Principia has had several contracts to study this problem in recent years, which have required reviewing the state-of-the-art, adopting appropriate mathematical descriptions, programming them into user routines in Abaqus, determining model parameters on the basis of some parts of the dams’ monitored histories, ensuring reliability using some other parts, and finally predicting the future evolution of the dams and their safety margins. The paper describes some of the above experience, including the programming of sophisticated non-isotropic swelling models, that must be compatible with cracking and other nonlinearities involved in concrete behaviour. The applications concentrate on two specific cases, an archgravity dam and a double-curvature arch dam, both with a long history of concrete swelling and which, interestingly, entailed different degrees of success in the modelling efforts

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The use of fly ash (FA) as an admixture to concrete is broadly extended for two main reasons: the reduction of costs that supposes the substitution of cement and the micro structural changes motivated by the mineral admixture. Regarding this second point, there is a consensus that considers that the ash generates a more compact concrete and a reduction in the size of the pore. However, the measure in which this contributes to the pozzolanic activity or as filler is not well defined. There is also no justification to the influence of the physical parameters, fineness of the grain and free water, in its behavior. This work studies the use of FA as a partial substitute of the cement in concretes of different workability (dry and wet) and the influence in the reactivity of the ash. The concrete of dry consistency which serves as reference uses a cement dose of 250 Kg/m 3 and the concrete of fluid consistency utilized a dose of cement of 350 Kg/m 3 . Two trademark of Portland Cement Type 1 were used. The first reached the resistant class for its fineness of grain and the second one for its composition. Moreover, three doses of FA have been used, and the water/binder ratio was constant in all the mixtures. We have studied the mechanical properties and the micro-structure of the concretes by means of compressive strength tests, mercury intrusion porosimetry (MIP) and thermal analysis (TA). The results of compressive strength tests allow us to observe that concrete mixtures with cements of the same classification and similar dosage of binder do not present the same mechanical behavior. These results show that the effective water/binder ratio has a major role in the development of the mechanical properties of concrete. The study of different dosages using TA, thermo-gravimetry and differential thermal analysis, revealed that the portlandite content is not restrictive in any of the dosages studied. Again, this proves that the rheology of the material influences the reaction rate and content of hydrated cement products. We conclude that the available free water is determinant in the efficiency of pozzolanic reaction. It is so that in accordance to the availability of free water, the ashes can react as an active admixture or simply change the porous distribution. The MIP shows concretes that do not exhibit significant changes in their mechanical behavior, but have suffered significant variation in their porous structure

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Around ten years ago investigation of technical and material construction in Ancient Roma has advanced in favour to obtain positive results. This process has been directed to obtaining some dates based in chemical composition, also action and reaction of materials against meteorological assaults or post depositional displacements. Plenty of these dates should be interpreted as a result of deterioration and damage in concrete material made in one landscape with some kind of meteorological characteristics. Concrete mixture like calcium and gypsum mortars should be analysed in laboratory test programs, and not only with descriptions based in reference books of Strabo, Pliny the Elder or Vitruvius. Roman manufacture was determined by weather condition, landscape, natural resources and of course, economic situation of the owner. In any case we must research the work in every facts of construction. On the one hand, thanks to chemical techniques like X-ray diffraction and Optical microscopy, we could know the granular disposition of mixture. On the other hand if we develop physical and mechanical techniques like compressive strength, capillary absorption on contact or water behaviour, we could know the reactions in binder and aggregates against weather effects. However we must be capable of interpret these results. Last year many analyses developed in archaeological sites in Spain has contributed to obtain different point of view, so has provide new dates to manage one method to continue the investigation of roman mortars. If we developed chemical and physical analysis in roman mortars at the same time, and we are capable to interpret the construction and the resources used, we achieve to understand the process of construction, the date and also the way of restoration in future.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Under-deck cable-stayed bridges are very effective structural systems for which the strong contribution of the stay cables under live loading allows for the design of very slender decks for persistent and transient loading scenarios. Their behaviour when subjected to seismic excitation is investigated herein and a set of design criteria are presented that relate to the type and arrangement of bearings, the number and configuration of struts, and the transverse distribution of stay cables. The nonlinear behaviour of these bridges when subject to both near-field and far-field accelerograms has been thoroughly investigated through the use of incremental dynamic analyses. An intensity measure that reflects the pertinent contributions to response when several vibration modes are activated was proposed and is shown to be effective for the analysis of this structural type. The under-deck cable-stay system contributes in a very positive manner to reducing the response when the bridges are subject to very strong seismic excitation. For such scenarios, the reduction in the stiffness of the deck because of crack formation, when prestressed concrete decks are used, mobilises the cable system and enhances the overall performance of the system. Sets of natural accelerograms that are compliant with the prescriptions of Eurocode 8 were also applied to propose a set of design criteria for this bridge type in areas prone to earthquakes. Particular attention is given to outlining the optimal strategies for the deployment of bearings

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Corrosion of reinforcing steel in concrete due to chloride ingress is one of the main causes of the deterioration of reinforced concrete structures. Structures most affected by such a corrosion are marine zone buildings and structures exposed to de-icing salts like highways and bridges. Such process is accompanied by an increase in volume of the corrosión products on the rebarsconcrete interface. Depending on the level of oxidation, iron can expand as much as six times its original volume. This increase in volume exerts tensile stresses in the surrounding concrete which result in cracking and spalling of the concrete cover if the concrete tensile strength is exceeded. The mechanism by which steel embedded in concrete corrodes in presence of chloride is the local breakdown of the passive layer formed in the highly alkaline condition of the concrete. It is assumed that corrosion initiates when a critical chloride content reaches the rebar surface. The mathematical formulation idealized the corrosion sequence as a two-stage process: an initiation stage, during which chloride ions penetrate to the reinforcing steel surface and depassivate it, and a propagation stage, in which active corrosion takes place until cracking of the concrete cover has occurred. The aim of this research is to develop computer tools to evaluate the duration of the service life of reinforced concrete structures, considering both the initiation and propagation periods. Such tools must offer a friendly interface to facilitate its use by the researchers even though their background is not in numerical simulation. For the evaluation of the initiation period different tools have been developed: Program TavProbabilidade: provides means to carry out a probability analysis of a chloride ingress model. Such a tool is necessary due to the lack of data and general uncertainties associated with the phenomenon of the chloride diffusion. It differs from the deterministic approach because it computes not just a chloride profile at a certain age, but a range of chloride profiles for each probability or occurrence. Program TavProbabilidade_Fiabilidade: carries out reliability analyses of the initiation period. It takes into account the critical value of the chloride concentration on the steel that causes breakdown of the passive layer and the beginning of the propagation stage. It differs from the deterministic analysis in that it does not predict if the corrosion is going to begin or not, but to quantifies the probability of corrosion initiation. Program TavDif_1D: was created to do a one dimension deterministic analysis of the chloride diffusion process by the finite element method (FEM) which numerically solves Fick’second Law. Despite of the different FEM solver already developed in one dimension, the decision to create a new code (TavDif_1D) was taken because of the need to have a solver with friendly interface for pre- and post-process according to the need of IETCC. An innovative tool was also developed with a systematic method devised to compare the ability of the different 1D models to predict the actual evolution of chloride ingress based on experimental measurements, and also to quantify the degree of agreement of the models with each others. For the evaluation of the entire service life of the structure: a computer program has been developed using finite elements method to do the coupling of both service life periods: initiation and propagation. The program for 2D (TavDif_2D) allows the complementary use of two external programs in a unique friendly interface: • GMSH - an finite element mesh generator and post-processing viewer • OOFEM – a finite element solver. This program (TavDif_2D) is responsible to decide in each time step when and where to start applying the boundary conditions of fracture mechanics module in function of the amount of chloride concentration and corrosion parameters (Icorr, etc). This program is also responsible to verify the presence and the degree of fracture in each element to send the Information of diffusion coefficient variation with the crack width. • GMSH - an finite element mesh generator and post-processing viewer • OOFEM – a finite element solver. The advantages of the FEM with the interface provided by the tool are: • the flexibility to input the data such as material property and boundary conditions as time dependent function. • the flexibility to predict the chloride concentration profile for different geometries. • the possibility to couple chloride diffusion (initiation stage) with chemical and mechanical behavior (propagation stage). The OOFEM code had to be modified to accept temperature, humidity and the time dependent values for the material properties, which is necessary to adequately describe the environmental variations. A 3-D simulation has been performed to simulate the behavior of the beam on both, action of the external load and the internal load caused by the corrosion products, using elements of imbedded fracture in order to plot the curve of the deflection of the central region of the beam versus the external load to compare with the experimental data.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Self-consciousness implies not only self or group recognition, but also real knowledge of one’s own identity. Self-consciousness is only possible if an individual is intelligent enough to formulate an abstract self-representation. Moreover, it necessarily entails the capability of referencing and using this elf-representation in connection with other cognitive features, such as inference, and the anticipation of the consequences of both one’s own and other individuals’ acts. In this paper, a cognitive architecture for self-consciousness is proposed. This cognitive architecture includes several modules: abstraction, self-representation, other individuals'representation, decision and action modules. It includes a learning process of self-representation by direct (self-experience based) and observational learning (based on the observation of other individuals). For model implementation a new approach is taken using Modular Artificial Neural Networks (MANN). For model testing, a virtual environment has been implemented. This virtual environment can be described as a holonic system or holarchy, meaning that it is composed of autonomous entities that behave both as a whole and as part of a greater whole. The system is composed of a certain number of holons interacting. These holons are equipped with cognitive features, such as sensory perception, and a simplified model of personality and self-representation. We explain holons’ cognitive architecture that enables dynamic self-representation. We analyse the effect of holon interaction, focusing on the evolution of the holon’s abstract self-representation. Finally, the results are explained and analysed and conclusions drawn.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

El hormigón es uno de los materiales de construcción más empleados en la actualidad debido a sus buenas prestaciones mecánicas, moldeabilidad y economía de obtención, entre otras ventajas. Es bien sabido que tiene una buena resistencia a compresión y una baja resistencia a tracción, por lo que se arma con barras de acero para formar el hormigón armado, material que se ha convertido por méritos propios en la solución constructiva más importante de nuestra época. A pesar de ser un material profusamente utilizado, hay aspectos del comportamiento del hormigón que todavía no son completamente conocidos, como es el caso de su respuesta ante los efectos de una explosión. Este es un campo de especial relevancia, debido a que los eventos, tanto intencionados como accidentales, en los que una estructura se ve sometida a una explosión son, por desgracia, relativamente frecuentes. La solicitación de una estructura ante una explosión se produce por el impacto sobre la misma de la onda de presión generada en la detonación. La aplicación de esta carga sobre la estructura es muy rápida y de muy corta duración. Este tipo de acciones se denominan cargas impulsivas, y pueden ser hasta cuatro órdenes de magnitud más rápidas que las cargas dinámicas impuestas por un terremoto. En consecuencia, no es de extrañar que sus efectos sobre las estructuras y sus materiales sean muy distintos que las que producen las cargas habitualmente consideradas en ingeniería. En la presente tesis doctoral se profundiza en el conocimiento del comportamiento material del hormigón sometido a explosiones. Para ello, es crucial contar con resultados experimentales de estructuras de hormigón sometidas a explosiones. Este tipo de resultados es difícil de encontrar en la literatura científica, ya que estos ensayos han sido tradicionalmente llevados a cabo en el ámbito militar y los resultados obtenidos no son de dominio público. Por otra parte, en las campañas experimentales con explosiones llevadas a cabo por instituciones civiles el elevado coste de acceso a explosivos y a campos de prueba adecuados no permite la realización de ensayos con un elevado número de muestras. Por este motivo, la dispersión experimental no es habitualmente controlada. Sin embargo, en elementos de hormigón armado sometidos a explosiones, la dispersión experimental es muy acusada, en primer lugar, por la propia heterogeneidad del hormigón, y en segundo, por la dificultad inherente a la realización de ensayos con explosiones, por motivos tales como dificultades en las condiciones de contorno, variabilidad del explosivo, o incluso cambios en las condiciones atmosféricas. Para paliar estos inconvenientes, en esta tesis doctoral se ha diseñado un novedoso dispositivo que permite ensayar hasta cuatro losas de hormigón bajo la misma detonación, lo que además de proporcionar un número de muestras estadísticamente representativo, supone un importante ahorro de costes. Con este dispositivo se han ensayado 28 losas de hormigón, tanto armadas como en masa, de dos dosificaciones distintas. Pero además de contar con datos experimentales, también es importante disponer de herramientas de cálculo para el análisis y diseño de estructuras sometidas a explosiones. Aunque existen diversos métodos analíticos, hoy por hoy las técnicas de simulación numérica suponen la alternativa más avanzada y versátil para el cálculo de elementos estructurales sometidos a cargas impulsivas. Sin embargo, para obtener resultados fiables es crucial contar con modelos constitutivos de material que tengan en cuenta los parámetros que gobiernan el comportamiento para el caso de carga en estudio. En este sentido, cabe destacar que la mayoría de los modelos constitutivos desarrollados para el hormigón a altas velocidades de deformación proceden del ámbito balístico, donde dominan las grandes tensiones de compresión en el entorno local de la zona afectada por el impacto. En el caso de los elementos de hormigón sometidos a explosiones, las tensiones de compresión son mucho más moderadas, siendo las tensiones de tracción generalmente las causantes de la rotura del material. En esta tesis doctoral se analiza la validez de algunos de los modelos disponibles, confirmando que los parámetros que gobiernan el fallo de las losas de hormigón armado ante explosiones son la resistencia a tracción y su ablandamiento tras rotura. En base a los resultados anteriores se ha desarrollado un modelo constitutivo para el hormigón ante altas velocidades de deformación, que sólo tiene en cuenta la rotura por tracción. Este modelo parte del de fisura cohesiva embebida con discontinuidad fuerte, desarrollado por Planas y Sancho, que ha demostrado su capacidad en la predicción de la rotura a tracción de elementos de hormigón en masa. El modelo ha sido modificado para su implementación en el programa comercial de integración explícita LS-DYNA, utilizando elementos finitos hexaédricos e incorporando la dependencia de la velocidad de deformación para permitir su utilización en el ámbito dinámico. El modelo es estrictamente local y no requiere de remallado ni conocer previamente la trayectoria de la fisura. Este modelo constitutivo ha sido utilizado para simular dos campañas experimentales, probando la hipótesis de que el fallo de elementos de hormigón ante explosiones está gobernado por el comportamiento a tracción, siendo de especial relevancia el ablandamiento del hormigón. Concrete is nowadays one of the most widely used building materials because of its good mechanical properties, moldability and production economy, among other advantages. As it is known, it has high compressive and low tensile strengths and for this reason it is reinforced with steel bars to form reinforced concrete, a material that has become the most important constructive solution of our time. Despite being such a widely used material, there are some aspects of concrete performance that are not yet fully understood, as it is the case of its response to the effects of an explosion. This is a topic of particular relevance because the events, both intentional and accidental, in which a structure is subjected to an explosion are, unfortunately, relatively common. The loading of a structure due to an explosive event occurs due to the impact of the pressure shock wave generated in the detonation. The application of this load on the structure is very fast and of very short duration. Such actions are called impulsive loads, and can be up to four orders of magnitude faster than the dynamic loads imposed by an earthquake. Consequently, it is not surprising that their effects on structures and materials are very different than those that cause the loads usually considered in engineering. This thesis broadens the knowledge about the material behavior of concrete subjected to explosions. To that end, it is crucial to have experimental results of concrete structures subjected to explosions. These types of results are difficult to find in the scientific literature, as these tests have traditionally been carried out by armies of different countries and the results obtained are classified. Moreover, in experimental campaigns with explosives conducted by civil institutions the high cost of accessing explosives and the lack of proper test fields does not allow for the testing of a large number of samples. For this reason, the experimental scatter is usually not controlled. However, in reinforced concrete elements subjected to explosions the experimental dispersion is very pronounced. First, due to the heterogeneity of concrete, and secondly, because of the difficulty inherent to testing with explosions, for reasons such as difficulties in the boundary conditions, variability of the explosive, or even atmospheric changes. To overcome these drawbacks, in this thesis we have designed a novel device that allows for testing up to four concrete slabs under the same detonation, which apart from providing a statistically representative number of samples, represents a significant saving in costs. A number of 28 slabs were tested using this device. The slabs were both reinforced and plain concrete, and two different concrete mixes were used. Besides having experimental data, it is also important to have computational tools for the analysis and design of structures subjected to explosions. Despite the existence of several analytical methods, numerical simulation techniques nowadays represent the most advanced and versatile alternative for the assessment of structural elements subjected to impulsive loading. However, to obtain reliable results it is crucial to have material constitutive models that take into account the parameters that govern the behavior for the load case under study. In this regard it is noteworthy that most of the developed constitutive models for concrete at high strain rates arise from the ballistic field, dominated by large compressive stresses in the local environment of the area affected by the impact. In the case of concrete elements subjected to an explosion, the compressive stresses are much more moderate, while tensile stresses usually cause material failure. This thesis discusses the validity of some of the available models, confirming that the parameters governing the failure of reinforced concrete slabs subjected to blast are the tensile strength and softening behaviour after failure. Based on these results we have developed a constitutive model for concrete at high strain rates, which only takes into account the ultimate tensile strength. This model is based on the embedded Cohesive Crack Model with Strong Discontinuity Approach developed by Planas and Sancho, which has proved its ability in predicting the tensile fracture of plain concrete elements. The model has been modified for its implementation in the commercial explicit integration program LS-DYNA, using hexahedral finite elements and incorporating the dependence of the strain rate, to allow for its use in dynamic domain. The model is strictly local and does not require remeshing nor prior knowledge of the crack path. This constitutive model has been used to simulate two experimental campaigns, confirming the hypothesis that the failure of concrete elements subjected to explosions is governed by their tensile response, being of particular relevance the softening behavior of concrete.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This work shows a numerical procedure for bond between indented wires and concrete, and the coupled splitting of the concrete. The bond model is an interface, non-associative, plasticity model. It is coupled with a cohesive fracture model for concrete to take into account the splitting of such concrete. The radial component of the prestressing force, increased by Poisson’s effect, may split the surrounding concrete, decreasing the wire confinement and diminishing the bonding. The combined action of the bond and the splitting is studied with the proposed model. The results of the numerical model are compared with the results of a series of tests, such as those which showed splitting induced by the bond between wire and concrete. Tests with different steel indentation depths were performed. The numerical procedure accurately reproduces the experimental records and improves knowledge of this complex process.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Las reformas de agua en países en desarrollo suelen llevarse a cabo junto con cambios institucionales más profundos o, incluso, acompañadas de cambios constitucionales o de régimen político. Por lo tanto, los marcos institucionales adaptados a países gobernados sujetos al estado de derecho pueden no ser apropiados para contextos gobernados fundamentalmente, al menos en sus inicios, por instituciones informales o poco maduras. Esta tesis toma las reformas de agua como punto de partida y pretende contribuir a la literatura mediante una serie de análisis empíricos tanto del ámbito general como del plano individual o sujeto personal de la política del agua. En el ámbito general, el foco se pone en los factores que explican el fallo de la acción colectiva en dos contextos diferentes: 1) en la implementación de la nueva Ley de Aguas de Nicaragua y 2) en el mantenimiento y revitalización de las instituciones de riego en Surinam. En el plano del individuo, la investigación se centra en las decisiones de los usuarios de los recursos y analiza el papel crítico de las variables sociales para la gestión de los recursos comunes. Para ello, el método de investigación utilizado es mixto, combinando el análisis de entrevistas, encuestas y experimentos. En el ámbito general, los resultados muestran que las principales barreras para la implementación de la nueva Ley de Aguas de Nicaragua podrían tener su reflejo en el lenguaje de la Ley y, por tanto, en la forma en la que se definen y configuran las instituciones incluidas en dicha Ley. Así, la investigación demuestra que la implementación de políticas no puede ser estudiada o entendida sin tener en cuenta tanto el diseño de la propia política como el marco socio-ecológico en el que se enmarca. El contexto específico de Nicaragua remarca la importancia de considerar tanto las instituciones formales como informales en los procesos de transición política. A pesar de que las reformas de agua requieren plazos largos para su implementación, el hecho de que exista una diferencia entre las reglas tal cual se definen formalmente y las reglas que operan en la realidad merece una mayor consideración en el diseño de políticas basadas fundamentalmente en instituciones formales. En el ámbito de la conducta individual, el análisis de la acción colectiva ofrece una serie de observaciones empíricas interesantes. En el caso de Nicaragua, los resultados indican que la intensidad de las relaciones sociales, el tipo de agentes dispuestos a proporcionar apoyo social y el nivel de confianza en la comunidad son factores que explican de manera significativa la participación en la comunidad. Sin embargo, el hecho de que la gestión colectiva de riego se produzca, en la mayoría de casos, en torno a lazos familiares sugiere que las variables de capital social críticas se definen en gran medida en la esfera familiar, siendo difícil que se extiendan fuera de estos nexos. El análisis experimental de los resultados de un juego de uso de recurso común y contribución al bien público muestra que las preferencias pro-sociales de los individuos y la heterogeneidad del grupo en términos de composición por sexo son factores que explican significativamente los resultados y las decisiones de apropiación a lo largo del juego. En términos del diseño de las políticas, es fundamental tener en cuenta las dinámicas de participación y uso de los recursos comunes de manera que los niveles de cooperación puedan mantenerse en el largo plazo, lo cual, como se observa en el caso de Surinam, no es siempre posible. Finalmente, el caso de Surinam es un ejemplo ilustrativo de los procesos de acción colectiva en economías en transición. El análisis del fallo de la acción colectiva en Surinam muestra que los procesos políticos vinculados al período colonial y de independencia explican en gran medida la falta de claridad en las reglas operacionales y colectivas que gobiernan la gestión de los sistemas de riego y drenaje. Los resultados empíricos sugieren que a pesar de que la acción colectiva para la provisión de los servicios de riego y drenaje estaba bien establecida bajo el régimen colonial, la auto-organización no prosperó en un contexto dependiente del apoyo externo y regido fundamentalmente por reglas diseñadas al nivel competencial del gobierno central. El sistema socio-ecológico que se desarrolló durante la transición post-colonial favoreció, así, la emergencia de comportamientos oportunistas, y posteriormente la inoperancia de los Water Boards (WBs) creados en la época colonial. En este sentido, cualquier intento por revitalizar los WBs y fomentar el desarrollo de la auto-organización de los usuarios necesitará abordar los problemas relacionados con los patrones demográficos, incluyendo la distribución de la tierra, el diseño de instituciones y la falta de confianza en el gobierno, además de las inversiones típicas en infraestructura y sistemas de información hidrológicos. El liderazgo del gobierno, aportando empuje de arriba-abajo, es, además, otro elemento imprescindible en Surinam. ABSTRACT Water reforms in developing countries take place along deeper institutional and even constitutional. Therefore, institutional frameworks that might result in positive outcomes in countries governed by the rule of law might not fit in contexts governed mainly by informal or immature institutions. This thesis takes water reforms as the starting point and aims to contribute to the literature by presenting several conceptual and empirical analyses at both general and individual levels. At the general national level, the focus is on the factors explaining failure of collective action in two different settings: 1) in the implementation of the new Nicaraguan Water Law and 2) in sustaining and revitalizing irrigation institutions in Suriname. At the individual level, the research focuses on the actions of resource users and analyzes the critical role of social variables for common pool resources management. For this purpose, the research presented in this thesis makes use of a mixed-method approach, combining interviews, surveys and experimental methods. Overall, the results show that major barriers for the implementation of the new Nicaraguan Water Law have its reflection on the language of the Law and, therefore, on the way institutions are defined and configured. In this sense, our study shows that implementation cannot fruitfully be studied and understood without taking into account both the policy design and the social-ecological context in which it is framed. The specific setting of Nicaragua highlights the relevance of considering both formal and informal institutions when promoting policy transitions. Despite the unquestionable fact that water reforms implementation needs long periods of time, there is still a gap between the rules on paper and the rules on the ground that deserves further attention when proposing policy changes on the basis of formal institutions. At the level of the individual agent, the analysis of collective action provides a number of interesting empirical insights. In the case of Nicaragua, I found that the intensity of social networks, the type of agents willing to provide social support and the level of trust in the community are all significant factors in explaining collective action at community level. However, the fact that most collective irrigation relies on family ties suggests that critical social capital variables might be defined within the family sphere and making it difficult to go beyond it. Experimental research combining a common pool resource and a public good game in Nicaragua shows that individuals’ pro-social traits and group heterogeneity in terms of sex composition are significant variables in explaining efficiency outcomes and effort decisions along the game. Thus, with regard to policy design, it is fundamental to consider carefully the dynamics of agents' participation and use of common pool resources, for sustaining cooperation in the long term, which, as seen in the case and Surinam, is not always possible. The case of Suriname provides a rich setting for the analysis of collective action in transition economies. The analysis of decay of collective irrigation in Suriname shows that the lack of clear operational and collective choice rules appear to be rooted in deeper political processes that date back to the colonial period. The empirical findings suggest that despite collective action for the provision of irrigation and drainage services was well established during the colonial period, self-organization did not flourish in a context governed by colonial state-crafted rules and mostly dependent on external support. The social-ecological system developed during the post-colonial transition process favored the emergence of opportunistic behavior. In this respect, any attempt to revitalize WBs and support self-organization will need to tackle the problems derived from demographic patterns, including land allocation, institutions design and government distrust, in addition to the typical investments in both physical infrastructure and hydrological information systems. The leadership role of the government, acting as a top-down trigger, is another essential element in Suriname.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A methodology has been developed for characterising the mechanical behaviour of concrete, based on the damaged plasticity model, enriched with a user subroutine (V)USDFLD in order to capture better the ductility of the material under moderate confining pressures. The model has been applied in the context of the international benchmark IRIS_2012, organised by the OECD/NEA/CSNI Nuclear Energy Agency, dealing with impacts of rigid and deformable missiles against reinforced concrete targets. A slightly modified version of the concrete damaged plasticity model was used to represent the concrete. The simulation results matched very well the observations made during the actual tests. Particularly successful predictions involved the energy spent by the rigid missile in perforating the target, the crushed length of the deformable missile, the crushed and cracked areas of the concrete target, and the values of the strains recorded at a number of locations in the concrete slab.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The study of sulfate attack in concrete is considered vital for the preservation of the structural integrity of constructions. Its aggressive behaviour causes degradation of the cement matrix which changes the initial properties of the material. In this article, the sulfate resistance of concrete is studied. To that goal, four different concrete mixes were made with sulphur resistant cement. The concretes were tested for compressive strength, transport capacity of sulfates and microstructural properties. An experimental program was proposed in which the concrete samples were submerged in sodium sulphate (Na2SO4) solution. The obtained results were compared with reference values of concretes cured in calcium hydroxide [Ca(OH)2]. According to the results the concrete with ground granulated blast-furnace slag presented the best behavior when exposed to sodium sulphate (Na2SO4) solution. El estudio del ataque de sulfatos en el hormigón se considera de gran importancia para la conservación de la integridad estructural de las construcciones. Su agresividad se basa en la degradación de la matriz cementicia modificando las características iniciales de diseño. En el presente trabajo se estudia la resistencia del hormigón al ataque de sulfatos provenientes de sulfato sódico (Na2SO4). Para llevar a cabo la investigación se diseñaron cuatro dosificaciones de hormigón empleando cementos sulforresistentes y adiciones minerales. Se llevó a cabo una propuesta experimental donde las muestras de hormigón se sumergieron en disolución de sulfato sódico (Na2SO4) de concentración 1M. Posteriormente se realizaron ensayos de resistencia mecánica, capacidad de transporte de sulfatos y propiedades microestructurales, a distintas edades. Los resultados obtenidos se compararon con valores de referencia de mezclas de hormigón curadas expuestas a hi-dróxido cálcico [Ca(OH)2]. De acuerdo a los resultados obtenidos, el hormigón con escoria de alto horno presentó las mejores características de durabilidad frente a sulfatos provenientes de sulfato sódico

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In order to show the choice of transparency as the guiding principle of the accreditation process, the article evaluates its influence on the fundamental subprocess of self-evaluation, thereby confirming that transparency is an essential tool for continuous improvement of academic processes and those of educational quality management. It fosters educational innovation and permits the sustainability of the continuous accreditation process over time, resulting in greater probabilities of university self-regulation through systemization of the process, with the objective of continuous improvement of university degree programs. The article analyzes the influence of transparency on each activity of the self-evaluation process according to the Peruvian accreditation model prepared under the total quality approach, as a reference for other accreditation models, proposing concrete transparency actions and evaluating its influence on the stakeholder groups in the self-evaluation process, as well as on the efficiency and effectiveness of the process. It is concluded that transparency has a positive influence on the training of human capital and the formation of the university?s organizational culture, facilitating dissemination, understanding and involvement of the stakeholder groups in the continuous improvement of accreditation activities and increasing their acceptance of change and commitment to the process. It is confirmed that transparency contributes toward increasing the efficiency index of the self-evaluation process by reducing operating costs through adequate, accessible, timely contribution of information by the stakeholders and through the optimization of the time spent gathering relevant information. In addition, it is concluded that transparency contributes toward increasing the effectiveness index of self-evaluation by facilitating the achievement of its objectives through synthetic, useful, reliable interpretation of the education situation and the formulation of feasible improvement plans based on the adequacy, relevance, visibility, pertinence and truthfulness of the information analyzed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

El auge que ha surgido en los últimos años por la reparación de edificios y estructuras construidas con hormigón ha llevado al desarrollo de morteros de reparación cada vez más tecnológicos. En el desarrollo de estos morteros por parte de los fabricantes, surge la disyuntiva en el uso de los polímeros en sus formulaciones, por no encontrarse justificado en ocasiones el trinomio prestaciones/precio/aplicación. En esta tesis se ha realizado un estudio exhaustivo para la justificación de la utilización de estos morteros como morteros de reparación estructural como respuesta a la demanda actual disponiéndolo en tres partes: En la primera parte se realizó un estudio del arte de los morteros y sus constituyentes. El uso de los morteros se remonta a la antigüedad, utilizándose como componentes yeso y cal fundamentalmente. Los griegos y romanos desarrollaron el concepto de morteros de cal, introduciendo componentes como las puzolanas, cales hidraúlicas y áridos de polvo de mármol dando origen a morteros muy parecidos a los hormigones actuales. En la edad media y renacimiento se perdió la tecnología desarrollada por los romanos debido al extenso uso de la piedra en las construcciones civiles, defensivas y religiosas. Hubo que esperar hasta el siglo XIX para que J. Aspdin descubriese el actual cemento como el principal compuesto hidraúlico. Por último y ya en el siglo XX con la aparición de moléculas tales como estireno, melanina, cloruro de vinilo y poliésteres se comenzó a desarrollar la industria de los polímeros que se añadieron a los morteros dando lugar a los “composites”. El uso de polímeros en matrices cementantes dotan al mortero de propiedades tales como: adherencia, flexibilidad y trabajabilidad, como ya se tiene constancia desde los años 30 con el uso de caucho naturales. En la actualidad el uso de polímeros de síntesis (polivinialacetato, estireno-butadieno, viniacrílico y resinas epoxi) hacen que principalmente el mortero tenga mayor resistencia al ataque del agua y por lo tanto aumente su durabilidad ya que se minimizan todas las reacciones de deterioro (hielo, humedad, ataque biológico,…). En el presente estudio el polímero que se utilizó fue en estado polvo: polímero redispersable. Estos polímeros están encapsulados y cuando se ponen en contacto con el agua se liberan de la cápsula formando de nuevo el gel. En los morteros de reparación el único compuesto hidraúlico que hay es el cemento y es el principal constituyente hoy en día de los materiales de construcción. El cemento se obtiene por molienda conjunta de Clínker y yeso. El Clínker se obtiene por cocción de una mezcla de arcillas y calizas hasta una temperatura de 1450-1500º C por reacción en estado fundente. Para esta reacción se deben premachacar y homogeneizar las materias primas extraídas de la cantera. Son dosificadas en el horno con unas proporciones tales que cumplan con unas relación de óxidos tales que permitan formar las fases anhidras del Clínker C3S, C2S, C3A y C4AF. De la hidratación de las fases se obtiene el gel CSH que es el que proporciona al cemento de sus propiedades. Existe una norma (UNE-EN 197-1) que establece la composición, especificaciones y tipos de cementos que se fabrican en España. La tendencia actual en la fabricación del cemento pasa por el uso de cementos con mayores contenidos de adiciones (cal, puzolana, cenizas volantes, humo de sílice,…) con el objeto de obtener cementos más sostenibles. Otros componentes que influyen en las características de los morteros son: - Áridos. En el desarrollo de los morteros se suelen usar naturales, bien calizos o silícicos. Hacen la función de relleno y de cohesionantes de la matriz cementante. Deben ser inertes - Aditivos. Son aquellos componentes del mortero que son dosificados en una proporción menor al 5%. Los más usados son los superplastificantes por su acción de reductores de agua que revierte en una mayor durabilidad del mortero. Una vez analizada la composición de los morteros, la mejora tecnológica de los mismos está orientada al aumento de la durabilidad de su vida en obra. La durabilidad se define como la capacidad que éste tiene de resistir a la acción del ambiente, ataques químicos, físicos, biológicos o cualquier proceso que tienda a su destrucción. Estos procesos dependen de factores tales como la porosidad del hormigón y de la exposición al ambiente. En cuanto a la porosidad hay que tener en cuenta la distribución de macroporos, mesoporos y microporos de la estructura del hormigón, ya que no todos son susceptibles de que se produzca el transporte de agentes deteriorantes, provocando tensiones internas en las paredes de los mismos y destruyendo la matriz cementante Por otro lado los procesos de deterioro están relacionados con la acción del agua bien como agente directo o como vehículo de transporte del agente deteriorante. Un ambiente que resulta muy agresivo para los hormigones es el marino. En este caso los procesos de deterioro están relacionados con la presencia de cloruros y de sulfatos tanto en el agua de mar como en la atmosfera que en combinación con el CO2 y O2 forman la sal de Friedel. El deterioro de las estructuras en ambientes marinos se produce por la debilitación de la matriz cementante y posterior corrosión de las armaduras que provocan un aumento de volumen en el interior y rotura de la matriz cementante por tensiones capilares. Otras reacciones que pueden producir estos efectos son árido-álcali y difusión de iones cloruro. La durabilidad de un hormigón también depende del tipo de cemento y su composición química (cementos con altos contenidos de adición son más resistentes), relación agua/cemento y contenido de cemento. La Norma UNE-EN 1504 que consta de 10 partes, define los productos para la protección y reparación de estructuras de hormigón, el control de calidad de los productos, propiedades físico-químicas y durables que deben cumplir. En esta Norma se referencian otras 65 normas que ofrecen los métodos de ensayo para la evaluación de los sistemas de reparación. En la segunda parte de esta Tesis se hizo un diseño de experimentos con diferentes morteros poliméricos (con concentraciones de polímero entre 0 y 25%), tomando como referencia un mortero control sin polímero, y se estudiaron sus propiedades físico-químicas, mecánicas y durables. Para mortero con baja proporción de polímero se recurre a sistemas monocomponentes y para concentraciones altas bicomponentes en la que el polímero está en dispersión acuosa. Las propiedades mecánicas medidas fueron: resistencia a compresión, resistencia a flexión, módulo de elasticidad, adherencia por tracción directa y expansión-retracción, todas ellas bajo normas UNE. Como ensayos de caracterización de la durabilidad: absorción capilar, resistencia a carbonatación y adherencia a tracción después de ciclos hielo-deshielo. El objeto de este estudio es seleccionar el mortero con mejor resultado general para posteriormente hacer una comparativa entre un mortero con polímero (cantidad optimizada) y un mortero sin polímero. Para seleccionar esa cantidad óptima de polímero a usar se han tenido en cuenta los siguientes criterios: el mortero debe tener una clasificación R4 en cuanto a prestaciones mecánicas al igual que para evaluar sus propiedades durables frente a los ciclos realizados, siempre teniendo en cuenta que la adición de polímero no puede ser elevada para hacer el mortero competitivo. De este estudio se obtuvieron las siguientes conclusiones generales: - Un mortero normalizado no cumple con propiedades para ser clasificado como R3 o R4. - Sin necesidad de polímero se puede obtener un mortero que cumpliría con R4 para gran parte de las características medidas - Es necesario usar relaciones a:c< 0.5 para conseguir morteros R4, - La adición de polímero mejora siempre la adherencia, abrasión, absorción capilar y resistencia a carbonatación - Las diferentes proporciones de polímero usadas siempre suponen una mejora tecnológica en propiedades mecánicas y de durabilidad. - El polímero no influye sobre la expansión y retracción del mortero. - La adherencia se mejora notablemente con el uso del polímero. - La presencia de polímero en los morteros mejoran las propiedades relacionadas con la acción del agua, por aumento del poder cementante y por lo tanto de la cohesión. El poder cementante disminuye la porosidad. Como consecuencia final de este estudio se determinó que la cantidad óptima de polímero para la segunda parte del estudio es 2.0-3.5%. La tercera parte consistió en el estudio comparativo de dos morteros: uno sin polímero (mortero A) y otro con la cantidad optimizada de polímero, concluida en la parte anterior (mortero B). Una vez definido el porcentaje de polímeros que mejor se adapta a los resultados, se plantea un nuevo esqueleto granular mejorado, tomando una nueva dosificación de tamaños de áridos, tanto para el mortero de referencia, como para el mortero con polímeros, y se procede a realizar los ensayos para su caracterización física, microestructural y de durabilidad, realizándose, además de los ensayos de la parte 1, mediciones de las propiedades microestructurales que se estudiaron a través de las técnicas de porosimetría de mercurio y microscopia electrónica de barrido (SEM); así como propiedades del mortero en estado fresco (consistencia, contenido de aire ocluido y tiempo final de fraguado). El uso del polímero frente a la no incorporación en la formulación del mortero, proporcionó al mismo de las siguientes ventajas: - Respecto a sus propiedades en estado fresco: El mortero B presentó mayor consistencia y menor cantidad de aire ocluido lo cual hace un mortero más trabajable y más dúctil al igual que más resistente porque al endurecer dejará menos huecos en su estructura interna y aumentará su durabilidad. Al tener también mayor tiempo de fraguado, pero no excesivo permite que la manejabilidad para puesta en obra sea mayor, - Respecto a sus propiedades mecánicas: Destacar la mejora en la adherencia. Es una de las principales propiedades que confiere el polímero a los morteros. Esta mayor adherencia revierte en una mejora de la adherencia al soporte, minimización de las posibles reacciones en la interfase hormigón-mortero y por lo tanto un aumento en la durabilidad de la reparación ejecutada con el mortero y por consecuencia del hormigón. - Respecto a propiedades microestructurales: la porosidad del mortero con polímero es menor y menor tamaño de poro critico susceptible de ser atacado por agentes externos causantes de deterioro. De los datos obtenidos por SEM no se observaron grandes diferencias - En cuanto a abrasión y absorción capilar el mortero B presentó mejor comportamiento como consecuencia de su menor porosidad y su estructura microscópica. - Por último el comportamiento frente al ataque de sulfatos y agua de mar, así como al frente de carbonatación, fue más resistente en el mortero con polímero por su menor permeabilidad y su menor porosidad. Para completar el estudio de esta tesis, y debido a la gran importancia que están tomando en la actualidad factores como la sostenibilidad se ha realizado un análisis de ciclo de vida de los dos morteros objeto de estudio de la segunda parte experimental.In recent years, the extended use of repair materials for buildings and structures made the development of repair mortars more and more technical. In the development of these mortars by producers, the use of polymers in the formulations is a key point, because sometimes this use is not justified when looking to the performance/price/application as a whole. This thesis is an exhaustive study to justify the use of these mortars as a response to the current growing demand for structural repair. The thesis is classified in three parts:The first part is the study of the state of the art of mortars and their constituents.In ancient times, widely used mortars were based on lime and gypsum. The Greeks and Romans developed the concept of lime mortars, introducing components such as pozzolans, hydraulic limes and marble dust as aggregates, giving very similar concrete mortars to the ones used currently. In the middle Age and Renaissance, the technology developed by the Romans was lost, due to the extensive use of stone in the civil, religious and defensive constructions. It was not until the 19th century, when J. Aspdin discovered the current cement as the main hydraulic compound. Finally in the 20th century, with the appearance of molecules such as styrene, melanin, vinyl chloride and polyester, the industry began to develop polymers which were added to the binder to form special "composites".The use of polymers in cementitious matrixes give properties to the mortar such as adhesion, Currently, the result of the polymer synthesis (polivynilacetate, styrene-butadiene, vynilacrylic and epoxy resins) is that mortars have increased resistance to water attack and therefore, they increase their durability since all reactions of deterioration are minimised (ice, humidity, biological attack,...). In the present study the polymer used was redispersible polymer powder. These polymers are encapsulated and when in contact with water, they are released from the capsule forming a gel.In the repair mortars, the only hydraulic compound is the cement and nowadays, this is the main constituent of building materials. The current trend is centered in the use of higher contents of additions (lime, pozzolana, fly ash, silica, silica fume...) in order to obtain more sustainable cements. Once the composition of mortars is analyzed, the technological improvement is centred in increasing the durability of the working life. Durability is defined as the ability to resist the action of the environment, chemical, physical, and biological attacks or any process that tends to its destruction. These processes depend on factors such as the concrete porosity and the environmental exposure. In terms of porosity, it be considered, the distribution of Macropores and mesopores and pores of the concrete structure, since not all of them are capable of causing the transportation of damaging agents, causing internal stresses on the same walls and destroying the cementing matrix.In general, deterioration processes are related to the action of water, either as direct agent or as a transport vehicle. Concrete durability also depends on the type of cement and its chemical composition (cement with high addition amounts are more resistant), water/cement ratio and cement content. The standard UNE-EN 1504 consists of 10 parts and defines the products for the protection and repair of concrete, the quality control of products, physical-chemical properties and durability. Other 65 standards that provide the test methods for the evaluation of repair systems are referenced in this standard. In the second part of this thesis there is a design of experiments with different polymer mortars (with concentrations of polymer between 0 and 25%), taking a control mortar without polymer as a reference and its physico-chemical, mechanical and durable properties were studied. For mortars with low proportion of polymer, 1 component systems are used (powder polymer) and for high polymer concentrations, water dispersion polymers are used. The mechanical properties measured were: compressive strength, flexural strength, modulus of elasticity, adhesion by direct traction and expansion-shrinkage, all of them under standards UNE. As a characterization of the durability, following tests are carried out: capillary absorption, resistance to carbonation and pull out adhesion after freeze-thaw cycles. The target of this study is to select the best mortar to make a comparison between mortars with polymer (optimized amount) and mortars without polymer. To select the optimum amount of polymer the following criteria have been considered: the mortar must have a classification R4 in terms of mechanical performance as well as in durability properties against the performed cycles, always bearing in mind that the addition of polymer cannot be too high to make the mortar competitive in price. The following general conclusions were obtained from this study: - A standard mortar does not fulfill the properties to be classified as R3 or R4 - Without polymer, a mortar may fulfill R4 for most of the measured characteristics. - It is necessary to use relations w/c ratio < 0.5 to get R4 mortars - The addition of polymer always improves adhesion, abrasion, capillary absorption and carbonation resistance - The different proportions of polymer used always improve the mechanical properties and durability. - The polymer has no influence on the expansion and shrinkage of the mortar - Adhesion is improved significantly with the use of polymer. - The presence of polymer in mortars improves the properties related to the action of the water, by the increase of the cement power and therefore the cohesion. The cementitious properties decrease the porosity. As final result of this study, it was determined that the optimum amount of polymer for the second part of the study is 2.0 - 3.5%. The third part is the comparative study between two mortars: one without polymer (A mortar) and another with the optimized amount of polymer, completed in the previous part (mortar B). Once the percentage of polymer is defined, a new granular skeleton is defined, with a new dosing of aggregate sizes, for both the reference mortar, the mortar with polymers, and the tests for physical, microstructural characterization and durability, are performed, as well as trials of part 1, measurements of the microstructural properties that were studied by scanning electron microscopy (SEM) and mercury porosimetry techniques; as well as properties of the mortar in fresh State (consistency, content of entrained air and final setting time). The use of polymer versus non polymer mortar, provided the following advantages: - In fresh state: mortar with polymer presented higher consistency and least amount of entrained air, which makes a mortar more workable and more ductile as well as more resistant because hardening will leave fewer gaps in its internal structure and increase its durability. Also allow it allows a better workability because of the longer (not excessive) setting time. - Regarding the mechanical properties: improvement in adhesion. It is one of the main properties which give the polymer to mortars. This higher adhesion results in an improvement of adhesion to the substrate, minimization of possible reactions at the concrete-mortar interface and therefore an increase in the durability of the repair carried out with mortar and concrete. - Respect to microstructural properties: the porosity of mortar with polymer is less and with smaller pore size, critical to be attacked by external agents causing deterioration. No major differences were observed from the data obtained by SEM - In terms of abrasion and capillary absorption, polymer mortar presented better performance as a result of its lower porosity and its microscopic structure. - Finally behavior against attack by sulfates and seawater, as well as to carbonation, was better in the mortar with polymer because of its lower permeability and its lower porosity. To complete the study, due to the great importance of sustainability for future market facts, the life cycle of the two mortars studied was analysed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this paper the dynamics of axisymmetric, slender, viscous liquid bridges having volume close to the cylindrical one, and subjected to a small gravitational field parallel to the axis of the liquid bridge, is considered within the context of one-dimensional theories. Although the dynamics of liquid bridges has been treated through a numerical analysis in the inviscid case, numerical methods become inappropriate to study configurations close to the static stability limit because the evolution time, and thence the computing time, increases excessively. To avoid this difficulty, the problem of the evolution of these liquid bridges has been attacked through a nonlinear analysis based on the singular perturbation method and, whenever possible, the results obtained are compared with the numerical ones.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The study brings new insights on the hydrogen assisted stress corrosion on damage tolerance of a high-strength duplex stainless steel wire which concerns its potential use as active reinforcement for concrete prestressing. The adopted procedure was to experimentally state the effect of hydrogen on the damage tolerance of cylindrical smooth and precracked wire specimens exposed to stress corrosion cracking using the aggressive medium of the standard test developed by FIP (International Prestressing Federation). Stress corrosion testing, mechanical fracture tests and scanning electron microscopy analysis allowed the damage assessment, and explain the synergy between mechanical loading and environment action on the failure sequence of the wire. In presence of previous damage, hydrogen affects the wire behavior in a qualitative sense, consistently to the fracture anisotropy attributable to cold drawing, but it does not produce quantitative changes since the steel fully preserves its damage tolerance.