43 resultados para Surface mechanical properties


Relevância:

100.00% 100.00%

Publicador:

Resumo:

The objective of this study is to analyze the applicability of current models used for estimating the mechanical properties of conventional concrete to self-consolidating concrete (SCC). The mechanical properties evaluated are modulus of elasticity, tensile strength,and modulus of rupture. As part of the study, it was necessary to build an extensive database that included the proportions and mechanical properties of 627 mixtures from 138 different references. The same models that are currently used for calculating the mechanical properties of conventional concrete were applied to SCC to evaluate their applicability to this type of concrete. The models considered are the ACI 318, ACI 363R, and EC2. These are the most commonly used models worldwide. In the first part of the study, the overall behavior and adaptability of the different models to SCC is evaluated. The specific characterization parameters for each concrete mixture are used to calculate the various mechanical properties applying the different estimation models. The second part of the analysis consists of comparing the experimental results of all the mixtures included in the database with the estimated results to evaluate the applicability of these models to SCC. Various statistical procedures, such as regression analysis and residual analysis, are used to compare the predicted and measured properties. It terms of general applicability, the evaluated models are suitable for estimating the modulus of elasticity, tensile strength, and modulus of rupture of SCC. These models have a rather low sensitivity, however, and adjust well only to mean values. This is because the models use the compressive strength as the main variable to characterize the concrete and do not consider other variables that affect these properties.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel methodology based on instrumented indentation is developed to determine the mechanical properties of amorphous materials which present cohesive-frictional behaviour. The approach is based on the concept of a universal hardness equation, which results from the assumption of a characteristic indentation pressure proportional to the hardness. The actual universal hardness equation is obtained from a detailed finite element analysis of the process of sharp indentation for a very wide range of material properties, and the inverse problem (i.e. how to extract the elastic modulus, the compressive yield strength and the friction angle) from instrumented indentation is solved. The applicability and limitations of the novel approach are highlighted. Finally, the model is validated against experimental data in metallic and ceramic glasses as well as polymers, covering a wide range of amorphous materials in terms of elastic modulus, yield strength and friction angle.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The method reported in the literature to calculate the stress–strain curve of nuclear fuel cladding from ring tensile test is revisited in this paper and a new alternative is presented. In the former method, two universal curves are introduced under the assumption of small strain. In this paper it is shown that these curves are not universal, but material-dependent if geometric nonlinearity is taken into account. The new method is valid beyond small strains, takes geometric nonlinearity into consideration and does not need universal curves. The stress–strain curves in the hoop direction are determined by combining numerical calculations with experimental results in a convergent loop. To this end, ring tensile tests were performed in unirradiated hydrogen-charged samples. The agreement among the simulations and the experimental results is excellent for the range of concentrations tested (up to 2000 wppm hydrogen). The calculated stress–strain curves show that the mechanical properties do not depend strongly on the hydrogen concentration, and that no noticeable strain hardening occurs. However, ductility decreases with the hydrogen concentration, especially beyond 500 wppm hydrogen. The fractographic results indicate that as-received samples fail in a ductile fashion, whereas quasicleavage is bserved in the hydrogen-charged samples.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A novel methodology based on instrumented indentation was developed to characterize the mechanical properties of amorphous materials. The approach is based on the concept of a universal postulate that assumes the existence of a characteristic indentation pressure proportional to the hardness. This hypothesis was numerically validated. This method overcomes the limitation of the conventional indentation models (pile-up effects and pressure sensitivity materials).

Relevância:

100.00% 100.00%

Publicador:

Resumo:

On the efforts for rationalizing the production of peanuts in Spain, one of the objectives was to obtain a well adapted variety, suitable for mechanization. We tried to get information on the characteristics that would condition the suitability of a variety to mechanized production, principally mechanical harvesting. All the characters studied would then be taken into account in a breeding program.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

El objetivo del estudio es determinar el efecto de tratamiento de la madera de Pinus sylvestris con sustancias protectoras en las propiedades mecánicas. Para ello se utilizan 40 muestras de madera libre de defectos de Pinus sylvestris L. tratándose con protectores orgánicos (Vacsol Azure WR 2601) 50 con protectores hidrosolubles (Tanalith E 3492) y 40 muestras de control sin tratamiento. Se evaluó la resistencia mecánica a la flexión estática, módulo de elasticidad y la fuerza de compresión paralela a la fibra fueron comparados con madera no tratada. El análisis de regresión entre la penetración y la fuerza de compresión paralela se realizó con las muestras tratadas con conservante a base de agua. Resultados principales: Los resultados indican que la madera tratada (con cualquiera de los productos) presenta un aumento estadísticamente significativo de la resistencia mecánica en todas las tres características mecánicas. Los resultados obtenidos difieren de estudios anteriores llevada a cabo por otros autores. No hubo correlación entre la resistencia a la compresión en paralelo y el grado de impregnación de la madera con base de agua de cobre azoles. La explicación más probable para estos resultados se refiere a cambios en la presión durante el tratamiento. El uso de muestras de control no tratadas en lugar de las muestras tratadas sólo con agua es más probable para producir resultados significativos en los estudios de resistencia mecánica . La investigación pone de relieve que la madera tratada presenta un aumento estadísticamente significativo en el Modulo de Elasticidad, módulo de rotura a la flexión estática y resistencia a la compresión paralela. No hubo correlación entre la resistencia a la compresión en paralelo y el grado de impregnación con conservante hidrosoluble.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Nondestructive techniques are extensively researched for the measurement of physical properties of fruits related to quality. Optical properties can be applied mainly in the detection of those quality features which are related to the chemical composition of the fruit, color (in the VIS region) or chemical constituents (sugar, in the MR region) being the most important. The most relevant mechanical property of fruits is consistency, generally called firmness, and to date only techniques which are able to measure the mechanical properties of the fruit bulk tissue are used for its prediction. Fruits can be modelled as elastic bodies, or at least as partially elastic. Therefore, the measurement of some elastic constants of the fruit can be used for the evaluation of its firmness. The differences in the response to loading are relevant in studying a) fruit firmness and b) bruising susceptibility. Both have been modelled for selected fruit species and varieties.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Neuronal growth is a complex process involving many intra- and extracellular mechanisms which are collaborating conjointly to participate to the development of the nervous system. More particularly, the early neocortical development involves the creation of a multilayered structure constituted by neuronal growth (driven by axonal or dendritic guidance cues) as well as cell migration. The underlying mechanisms of such structural lamination not only implies important biochemical changes at the intracellular level through axonal microtubule (de)polymerization and growth cone advance, but also through the directly dependent stress/stretch coupling mechanisms driving them. Efforts have recently focused on modeling approaches aimed at accounting for the effect of mechanical tension or compression on the axonal growth and subsequent soma migration. However, the reciprocal influence of the biochemical structural evolution on the mechanical properties has been mostly disregarded. We thus propose a new model aimed at providing the spatially dependent mechanical properties of the axon during its growth. Our in-house finite difference solver Neurite is used to describe the guanosine triphosphate (GTP) transport through the axon, its dephosphorylation in guanosine diphosphate (GDP), and thus the microtubules polymerization. The model is calibrated against experimental results and the tensile and bending mechanical stiffnesses are ultimately inferred from the spatially dependent microtubule occupancy. Such additional information is believed to be of drastic relevance in the growth cone vicinity, where biomechanical mechanisms are driving axonal growth and pathfinding. More specifically, the confirmation of a lower stiffness in the distal axon ultimately participates in explaining the controversy associated to the tensile role of the growth cone.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Laser shock processing (LSP) is increasingly applied as an effective technology for the improvement of metallic materials mechanical properties in different types of components as a means of enhancement of their fatigue life behavior. As reported in previous contributions by the authors, a main effect resulting from the application of the LSP technique consists on the generation of relatively deep compression residual stresses fields into metallic components allowing an improved mechanical behaviour, explicitly the life improvement of the treated specimens against wear, crack growth and stress corrosion cracking. Additional results accomplished by the authors in the line of practical development of the LSP technique at an experimental level (aiming its integral assessment from an interrelated theoretical and experimental point of view) are presented in this paper. Concretely, experimental results on the residual stress profiles and associated mechanical properties modification successfully reached in typical materials under different LSP irradiation conditions are presented. In this case, the specific behavior of a widely used material in high reliability components (especially in nuclear and biomedical applications) as AISI 316L is analyzed, the effect of possible “in-service” thermal conditions on the relaxation of the LSP effects being specifically characterized. I.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This study analyses the variation of main physical-mechanical properties of wood along the longitudinal and radial directions of the tree for Abies alba Mill. growing in the Spanish Pyrenees. Small clear specimens were used to study the properties of volumetric shrinkage (VS), density (?), hardness (H), bending strength (MOR), modulus of elasticity (MOE), maximum compressive strength parallel to the grain (MCS) and impact strength (K). Several models of properties variation in the longitudinal and radial directions were analyzed. Main trends of variation of properties throughout the tree stem were identified although none of them could be fitted to predictive statistical models. Along the longitudinal direction, the properties studied followed a downward trend from the base to the crown, which was not significant in all cases, indicating that no differences in quality existed. Throughout the radial direction the trend is upward for the first 40-50 growth rings, after which it slopes downwards, more gently at first until rings 70-75 and then more steeply. This behaviour is related to variation in wood structure from the pith to the bark, depending on whether the wood is juvenile, sapwood or heartwood, and to wood maturity and microfibril angle. Authors encourage carrying further studies on other populations of A. alba in the Spanish Pyrenees to check if the trends found in this study apply to other provenances.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Long-length ultrafine-grained (UFG) Ti rods are produced by equal-channel angular pressing via the conform scheme (ECAP-C) at 200 °C, which is followed by drawing at 200 °C. The evolution of microstructure, macrotexture, and mechanical properties (yield strength, ultimate tensile strength, failure stress, uniform elongation, elongation to failure) of pure Ti during this thermo-mechanical processing is studied. Special attention is also paid to the effect of microstructure on the mechanical behavior of the material after macrolocalization of plastic flow. The number of ECAP-C passes varies in the range of 1–10. The microstructure is more refined with increasing number of ECAP-C passes. Formation of homogeneous microstructure with a grain/subgrain size of 200 nm and its saturation after 6 ECAP-C passes are observed. Strength properties increase with increasing number of ECAP passes and saturate after 6 ECAP-C passes to a yield strength of 973 MPa, an ultimate tensile strength of 1035 MPa, and a true failure stress of 1400 MPa (from 625, 750, and 1150 MPa in the as-received condition). The true strain at failure failure decreases after ECAP-C processing. The reduction of area and true strain to failure values do not decrease after ECAP-C processing. The sample after 6 ECAP-C passes is subjected to drawing at 200¯C resulting in reduction of a grain/subgrain size to 150 nm, formation of (10 View the MathML source1¯0) fiber texture with respect to the rod axis, and further increase of the yield strength up to 1190 MPa, the ultimate tensile strength up to 1230 MPa and the true failure stress up to 1600 MPa. It is demonstrated that UFG CP Ti has low resistance to macrolocalization of plastic deformation and high resistance to crack formation after necking.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A strategy is presented to optimize out-of-autoclave processing of quasi-isotropic carbon fiber-reinforced laminates. Square panels of 4.6 mm nominal thickness with very low porosity ð6 0:2%Þ were manufactured by compression molding at low pressure (0.2 MPa) by careful design of the temperature cycle to maximize the processing window. The mechanisms of void migration during processing were ascertained by means of X-ray microtomography and the effect of ply clustering on porosity and on void shape was explained. Finally, the effect of porosity and ply clustering on the compressive strength before and after impact was studied.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

One of the challenges of science and engineering nowadays is to develop new ways to supply energy in a sustainable and ecological mode. The fussion energy could be the final answer but a myriad of problems must be solved previously.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The EFDA-ITER programme for materials wants to develop new structural materials for future nuclear magnetic fusion reactors. In this context, special attention must be paid in the development of new composite materials that could support the hard working conditions of the nuclear fusion reactors: high temperature, high stresses, and high radiation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Assessment of laser shock processing effects on mechanical resistance of thin dissimilar laser welded joints