24 resultados para Plasma-materials interaction


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The interaction of high intensity X-ray lasers with matter is modeled. A collisional-radiative timedependent module is implemented to study radiation transport in matter from ultrashort and ultraintense X-ray bursts. Inverse bremsstrahlung absorption by free electrons, electron conduction or hydrodynamic effects are not considered. The collisional-radiative system is coupled with the electron distribution evolution treated with a Fokker-Planck approach with additional inelastic terms. The model includes spontaneous emission, resonant photoabsorption, collisional excitation and de-excitation, radiative recombination, photoionization, collisional ionization, three-body recombination, autoionization and dielectronic capture. It is found that for high densities, but still below solid, collisions play an important role and thermalization times are not short enough to ensure a thermal electron distribution. At these densities Maxwellian and non-Maxwellian electron distribution models yield substantial differences in collisional rates, modifying the atomic population dynamics.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Numerical investigations on mutual interactions between two spatially overlapping standing electromagnetic solitons in a cold unmagnetized plasma are reported. It is found that an initial state comprising of two overlapping standing solitons evolves into different end states, depending on the amplitudes of the two solitons and the phase difference between them. For small amplitude solitons with zero phase difference, we observe the formation of an oscillating bound state whose period depends on their initial separation. These results suggest the existence of a bound state made of two solitons in the relativistic cold plasma fluid model.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Raman scattering of Si nanowires (NWs) presents antenna effects. The electromagnetic resonance depends on the electromagnetic coupling of the system laser/NW/substrate. The antenna effect of the Raman signal was measured in individual NWs deposited on different substrates, and also free standing NWs in air. The one phonon Raman band in NWs can reach high intensities depending on the system configuration; values of Raman intensity per unit volume more than a few hundred times with respect to bulk substrate can be obtainedRaman scattering of Si nanowires (NWs) presents antenna effects. The electromagnetic resonance depends on the electromagnetic coupling of the system laser/NW/substrate. The antenna effect of the Raman signal was measured in individual NWs deposited on different substrates, and also free standing NWs in air. The one phonon Raman band in NWs can reach high intensities depending on the system configuration; values of Raman intensity per unit volume more than a few hundred times with respect to bulk substrate can be obtained

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nowadays, dispersion correction applied on layered semiconductors is a topic of interest. Among the known layered semiconductors, SnS2 polytypes are wide gap semiconductors with a van der Waals interaction between their layers, which could form good materials to be used in photovoltaic applications. The present work gives an approach to the SnS2 geometrical and electronic characterization using an empirical dispersion correction added to the Perdew–Burke–Ernzerhof functional and subsequent actualization of the electronic charge density using the screened hybrid Heyd–Scuseria–Ernzerhof functional using a density functional code. The obtained interlayer distance and band-gap are in good agreement with experimental values when van der Waals dispersion forces are included.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

El wolframio (W) y sus aleaciones se consideran los mejores candidatos para la construcción del divertor en la nueva generación de reactores de fusión nuclear. Este componente va a recibir las cargas térmicas más elevadas durante el funcionamiento del reactor ya que estará en contacto directo con el plasma. En los últimos años, después de un profundo análisis y siguiendo una estrategia de reducción de costes, la Organización de ITER tomó la decisión de construir el divertor integramente de wolframio desde el principio. Por ello, el wolframio no sólo actuará como material en contacto con el plasma (PFM), sino que también tendría aplicaciones estructurales. El wolframio, debido a sus excelentes propiedades termo-físicas, cumple todos los requerimientos para ser utilizado como PFM, sin embargo, su inherente fragilidad pone en peligro su uso estructural. Por tanto, uno de los principales objetivos de esta tesis es encontrar una aleación de wolframio con menor fragilidad. Durante éste trabajo, se realizó la caracterización microstructural y mecánica de diferentes materiales basados en wolframio. Sin embargo, ésta tarea es un reto debido a la pequeña cantidad de material suministrado, su reducido tamaño de grano y fragilidad. Por ello, para una correcta medida de todas las propiedades físicas y mecánicas se utilizaron diversas técnicas experimentales. Algunas de ellas se emplean habitualmente como la nanoindentación o los ensayos de flexión en tres puntos (TPB). Sin embargo, otras fueron especificamente desarrolladas e implementadas durante el desarrollo de esta tesis como es el caso de la medida real de la tenacidad de fractura en los materiales masivos, o de las medidas in situ de la tenacidad de fractura en las láminas delgadas de wolframio. Diversas composiciones de aleaciones de wolframio masivas (W-1% Y2O3, W-2% V-0.5% Y2O3, W-4% V-0.5% Y2O3, W-2% Ti-1% La2O3 y W-4% Ti-1% La2O3) se han estudiado y comparado con un wolframio puro producido en las mismas condiciones. Estas aleaciones, producidas por ruta pulvimetalúrgica de aleado mecánico (MA) y compactación isostática en caliente (HIP), fueron microstructural y mecánicamente caracterizadas desde 77 hasta 1473 K en aire y en alto vacío. Entre otras propiedades físicas y mecánicas se midieron la dureza, el módulo elástico, la resistencia a flexión y la tenacidad de fractura para todas las aleaciones. Finalmente se analizaron las superficies de fractura después de los ensayos de TPB para relacionar los micromecanismos de fallo con el comportamiento macroscópico a rotura. Los resultados obtenidos mostraron un comportamiento mecánico frágil en casi todo el intervalo de temperaturas y para casi todas las aleaciones sin mejoría de la temperatura de transición dúctil-frágil (DBTT). Con el fin de encontrar un material base wolframio con una DBTT más baja se realizó también un estudio, aún preliminar, de láminas delgadas de wolframio puro y wolframio dopado con 0.005wt.% potasio (K). Éstas láminas fueron fabricadas industrialmente mediante sinterizado y laminación en caliente y en frío y se sometieron posteriormente a un tratamiento térmico de recocido desde 1073 hasta 2673 K. Se ha analizado la evolución de su microestructura y las propiedades mecánicas al aumentar la temperatura de recocido. Los resultados mostraron la estabilización de los granos de wolframio con el incremento de la temperatura de recocido en las láminas delgadas de wolframio dopado con potasio. Sin embargo, es necesario realizar estudios adicionales para entender mejor la microstructura y algunas propiedades mecánicas de estos materiales, como la tenacidad de fractura. Tungsten (W) and tungsten-based alloys are considered to be the best candidate materials for fabricating the divertor in the next-generation nuclear fusion reactors. This component will experience the highest thermal loads during the operation of a reactor since it directly faces the plasma. In recent years, after thorough analysis that followed a strategy of cost reduction, the ITER Organization decided to built a full-tunsgten divertor before the first nuclear campaigns. Therefore, tungsten will be used not only as a plasma-facing material (PFM) but also in structural applications. Tungsten, due to its the excellent thermo-physical properties fulfils the requirements of a PFM, however, its use in structural applications is compromised due to its inherent brittleness. One of the objectives of this phD thesis is therefore, to find a material with improved brittleness behaviour. The microstructural and mechanical characterisation of different tunsgten-based materials was performed. However, this is a challenging task because of the reduced laboratory-scale size of the specimens provided, their _ne microstructure and their brittleness. Consequently, many techniques are required to ensure an accurate measurement of all the mechanical and physical properties. Some of the applied methods have been widely used such as nanoindentation or three-point bending (TPB) tests. However, other methods were specifically developed and implemented during this work such as the measurement of the real fracture toughness of bulk-tunsgten alloys or the in situ fracture toughness measurements of very thin tungsten foils. Bulk-tunsgten materials with different compositions (W-1% Y2O3, W-2% V- 0.5% Y2O3, W-4% V-0.5% Y2O3, W-2% Ti-1% La2O3 and W-4% Ti-1% La2O3) were studied and compared with pure tungsten processed under the same conditions. These alloys, produced by a powder metallurgical route of mechanical alloying (MA) and hot isostatic pressing (HIP), were microstructural and mechanically characterised from 77 to 1473 K in air and under high vacuum conditions. Hardness, elastic modulus, flexural strength and fracture toughness for all of the alloys were measured in addition to other physical and mechanical properties. Finally, the fracture surfaces after the TPB tests were analysed to correlate the micromechanisms of failure with the macroscopic behaviour. The results reveal brittle mechanical behaviour in almost the entire temperature range for the alloys and micromechanisms of failure with no improvement in the ductile-brittle transition temperature (DBTT). To continue the search of a tungsten material with lowered DBTT, a preliminary study of pure tunsgten and 0.005 wt.% potassium (K)-doped tungsten foils was also performed. These foils were industrially produced by sintering and hot and cold rolling. After that, they were annealed from 1073 to 2673 K to analyse the evolution of the microstructural and mechanical properties with increasing annealing temperature. The results revealed the stabilisation of the tungsten grains with increasing annealing temperature in the potassium-doped tungsten foil. However, additional studies need to be performed to gain a better understanding of the microstructure and mechanical properties of these materials such as fracture toughness.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

El ensamblado de nanotubos de carbono (CNT) como una fibra macroscópica en la cual están orientados preferentemente paralelos entre sí y al eje de la fibra, ha dado como resultado un nuevo tipo de fibra de altas prestaciones derivadas de la explotación eficiente de las propiedades axiales de los CNTs, y que tiene un gran número de aplicaciones potenciales. Fibras continuas de CNTs se produjeron en el Instituto IMDEA Materiales mediante el proceso de hilado directo durante la reacción de síntesis por deposición química de vapores. Uno de los objetivos de esta tesis es el estudio de la estructura de estas fibras mediante técnicas del estado del arte de difracción de rayos X de sincrotrón y la elaboración de un modelo estructural de dicho material. Mediciones texturales de adsorción de gases, análisis de micrografías de electrones y dispersión de rayos X de ángulo alto y bajo (WAXS/SAXS) indican que el material tiene una estructura mesoporosa con una distribución de tamaño de poros ancha derivada del amplio rango de separaciones entre manojos de CNTs, así como una superficie específica de 170m2/g. Los valores de dimensión fractal obtenidos mediante SAXS y análisis Barrett-Joyner-Halenda (BJH) de mediciones texturales coinciden en 2.4 y 2.5, respectivamente, resaltando el carácter de red de la estructura de dichas fibras. La estructura mesoporosa y tipo hilo de las fibra de CNT es accesible a la infiltración de moléculas externas (líquidos o polímeros). En este trabajo se estudian los cambios en la estructura multiescala de las fibras de CNTs al interactuar con líquidos y polímeros. Los efectos de la densificación en la estructura de fibras secas de CNT son estudiados mediante WAXS/SAXS. El tratamiento de densificación junta los manojos de la fibra (los poros disminuyen de tamaño), resultando en un incremento de la densidad de la fibra. Sin embargo, los dominios estructurales correspondientes a la transferencia de esfuerzo mecánica y carga eléctrica en los nanotubos no son afectados durante este proceso de densificación; como consecuencia no se produce un efecto sustancial en las propiedades mecánicas y eléctricas. Mediciones de SAXS and fibra de CNT antes y después de infiltración de líquidos confirman la penetración de una gran cantidad de líquidos que llena los poros internos de la fibra pero no se intercalan entre capas de nanotubos adyacentes. La infiltración de cadenas poliméricas de bajo peso molecular tiende a expandir los manojos en la fibra e incrementar el ángulo de apertura de los poros. Los resultados de SAXS indican que la estructura interna de la fibra en términos de la organización de las capas de tubos y su orientación no es afectada cuando las muestras consisten en fibras infiltradas con polímeros de alto peso molecular. La cristalización de varios polímeros semicristalinos es acelerada por la presencia de fibras de CNTs alineados y produce el crecimiento de una capa transcristalina normal a la superficie de la fibra. Esto es observado directamente mediante microscopía óptica polarizada, y detectado mediante calorimetría DSC. Las lamelas en la capa transcristalina tienen orientación de la cadena polimérica paralela a la fibra y por lo tanto a los nanotubos, de acuerdo con los patrones de WAXS. Esta orientación preferencial se sugiere como parte de la fuerza impulsora en la nucleación. La nucleación del dominio cristalino polimérico en la superficie de los CNT no es epitaxial. Ocurre sin haber correspondencia entre las estructuras cristalinas del polímero y los nanotubos. Estas observaciones contribuyen a la compresión del fenómeno de nucleación en CNTs y otros nanocarbonos, y sientan las bases para el desarrollo de composites poliméricos de gran escala basados en fibra larga de CNTs alineados. ABSTRACT The assembly of carbon nanotubes into a macroscopic fibre material where they are preferentially aligned parallel to each other and to the fibre axis has resulted in a new class of high-performance fibres, which efficiently exploits the axial properties of the building blocks and has numerous applications. Long, continuous CNT fibres were produced in IMDEA Materials Institute by direct fibre spinning from a chemical vapour deposition reaction. These fibres have a complex hierarchical structure covering multiple length scales. One objective of this thesis is to reveal this structure by means of state-of-the-art techniques such as synchrotron X-ray diffraction, and to build a model to link the fibre structural elements. Texture and gas absorption measurements, using electron microscopy, wide angle and small angle X-ray scattering (WAXS/SAXS), and pore size distribution analysis by Barrett-Joyner-Halenda (BJH), indicate that the material has a mesoporous structure with a wide pore size distribution arising from the range of fibre bundle separation, and a high surface area _170m2/g. Fractal dimension values of 2.4_2.5 obtained from the SAXS and BJH measurements highlight the network structure of the fibre. Mesoporous and yarn-like structure of CNT fibres make them accessible to the infiltration of foreign molecules (liquid or polymer). This work studies multiscale structural changes when CNT fibres interact with liquids and polymers. The effects of densification on the structure of dry CNT fibres were measured by WAXS/SAXS. The densification treatment brings the fibre bundles closer (pores become smaller), leading to an increase in fibre density. However, structural domains made of the load and charge carrying nanotubes are not affected; consequently, it has no substantial effect on mechanical and electrical properties. SAXS measurements on the CNT fibres before and after liquid infiltration imply that most liquids are able to fill the internal pores but not to intercalate between nanotubes. Successful infiltration of low molecular weight polymer chains tends to expand the fibre bundles and increases the pore-opening angle. SAXS results indicate that the inner structure of the fibre, in terms of the nanotube layer arrangement and the fibre alignment, are not largely affected when infiltrated with polymers of relatively high molecular weight. The crystallisation of a variety of semicrystalline polymers is accelerated by the presence of aligned fibres of CNTs and results in the growth of a transcrystalline layer perpendicular to the fibre surface. This can be observed directly under polarised optical microscope, and detected by the exothermic peaks during differential scanning calorimetry. The discussion on the driving forces for the enhanced nucleation points out the preferential chain orientation of polymer lamella with the chain axis parallel to the fibre and thus to the nanotubes, which is confirmed by two-dimensional WAXS patterns. A non-epitaxial polymer crystal growth habit at the CNT-polymer interface is proposed, which is independent of lattice matching between the polymer and nanotubes. These findings contribute to the discussion on polymer nucleation on CNTs and other nanocarbons, and their implication for the development of large polymer composites based on long and aligned fibres of CNTs.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work we have realized plasma diagnosis produced by Laser (LPP), by means of emission spectroscopy in a Laser Shock Processing (LSP). The LSP has been proposed as an alternative technology, competitive with classical surface treatments. The ionic species present in the plasma together with electron density and its temperature provide significant indicators of the degree of surface effect of the treated material. In order to analyze these indicators, we have realized spectroscopic studies of optical emission in the laser-generated plasmas in different situations. We have worked focusing on an aluminum sample (Al2024) in air and/or in LSP conditions (water flow) a Q-switched laser of Nd:YAG (λ = 1.06 μm, 10 ns of pulse duration, running at 10 Hz repetition rate). The pulse energy was set at 2,5 J per pulse. The electron density has been measured using, in every case, the Stark broadening of H Balmer α line (656.27 nm). In the case of the air, this measure has been contrasted with the value obtained with the line of 281.62 nm of Al II. Special attention has been paid to the self-absorption of the spectral lines used. The measures were realized with different delay times after the pulse of the laser (1–8 μs) and with a time window of 1 μs. In LSP the electron density obtained was between 1017 cm−3 for the shortest delays (4–6 μs), and 1016 cm−3 for the greatest delays (7,8 μs).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Las sociedades desarrolladas generan una gran cantidad de residuos, que necesitan una adecuada gestión. Esta problemática requiere, de este modo, una atención creciente por parte de la sociedad, debido a la necesidad de proteger el medio ambiente. En este sentido, los esfuerzos se centran en reducir al máximo la generación de residuos y buscar vías de aprovechamiento de aquellos que son inevitables, soluciones mucho más aconsejables desde el punto de vista técnico, ecológico y económico que su vertido o destrucción. Las industrias deben adoptar las medidas precisas para fomentar la reducción de estos residuos, desarrollar tecnologías limpias que permitan el ahorro de los recursos naturales que poseemos, y sobre todo buscar métodos de reutilización, reciclado, inertización y valorización de los residuos generados en su producción. La industria de la construcción es un campo muy receptivo para el desarrollo de nuevos materiales en los que incorporar estos residuos. La incorporación de diferentes residuos industriales en matrices cerámicas se plantea como una vía barata de fijar las diferentes especies metálicas presentes en transformación de rocas ornamentales, lodos de galvanización o metalúrgicos, etc. En todos los casos, la adición de estos residuos requiere su caracterización previa y la optimización de las condiciones de conformado y cocción en el caso de su incorporación a la arcilla cocida. Entre los residuos incorporados en materiales de construcción se encuentran las escorias de aluminio. La industria metalúrgica produce durante sus procesos de fusión diferentes tipos de escorias. Su reciclado es una de las líneas de interés para estas industrias. En el caso de las escorias de aluminio, su tratamiento inicial consiste en una recuperación del aluminio mediante métodos mecánicos seguido de un tratamiento químico, o plasma. Este método conduce a que la escoria final apenas contenga aluminio y sea rica en sales solubles lo que limita su almacenamiento en escombreras. La escoria es una mezcla de aluminio metal y productos no metálicos como óxidos, nitruros y carburos de aluminio, sales y otros óxidos metálicos. En este estudio se ha analizado la posibilidad de la adición de escorias de aluminio procedentes de la metalurgia secundaria en materiales de construcción, de forma que tras un procesado de las mismas permita la obtención de materiales compuestos de matriz cerámica. En la presente Tesis Doctoral se ha analizado la viabilidad técnica de la incorporación de las escorias de aluminio procedentes de la metalurgia secundaria en una matriz de arcilla cocida. Para ello se han aplicado diferentes tratamientos a la escoria y se han aplicado diferentes variables en su procesado como la energía de molienda o la temperatura de sinterizacion, además del contenido de escoria. Su compactación con agua entre el 5-10 %, secado y sinterización permite obtener piezas rectangulares de diverso tamaño. Desde el punto de vista del contenido de la escoria, se incorporó entre un 10 y 40% de escoria TT, es decir sometida una calcinación previa a 750ºC en aire. Los mejores resultados alcanzados corresponden a un contenido del 20% ESC TT, sinterizada a 980ºC, por cuanto altos contenidos en escoria condicen a piezas con corazón negro. Los productos obtenidos con la adición de 20% de escoria de aluminio a la arcilla, presentan una baja expansión tras sinterización, mejores propiedades físicas y mecánicas, y mayor conductividad térmica que los productos obtenidos con arcilla sin adiciones. Aumenta su densidad, disminuye su absorción y aumenta sus resistencias de flexión y compresión, al presentar una porosidad cerrada y una interacción escoria-matriz. En todos los casos se produce una exudación superficial de aluminio metálico, cuyo volumen está relacionado con la cantidad de escoria adicionada. Mediante la incorporación de este contenido de escoria, tras un tratamiento de disolución de sales y posterior calcinación (ESC TTQ), se mejoran las propiedades del material compuesto, no sólo sobre la de la escoria calcinada (ESC TT), sino también, sobre la escoria sin tratamiento (ESC). Si además, la adición del 20% de escoria añadida, está tratada, no sólo térmicamente sino también químicamente (ESC TTQ), éstas mejoran aún más las propiedades del material compuesto, siendo el producto más compacto, con menos poros, por lo que los valores de densidad son más elevados, menores son las absorciones y mayores resistencias de flexión y compresión, que los productos obtenidos con la adición de escoria sólo tratada térmicamente. Alcanzando valores de resistencias características a compresión del orden de 109 MPa. Los valores de conductividad térmica obtenidos también son mayores. Los ensayos tecnológicos con piezas de 160 x 30 x 5 mm y el material compuesto optimizado de arcilla+ 20%ESCTTQ, consistieron en la determinación de su expansión por humedad, eflorescencia y heladicidad, mostrando en general un mejor comportamiento que la arcilla sin adiciones. Así, se han obtenido nuevos materiales compuestos de matriz cerámica para la construcción, mejorando sus propiedades físicas, mecánicas y térmicas, utilizando escorias de aluminio procedentes de la metalurgia secundaria, como opción de valorización de estos residuos, evitando así, que se viertan a vertederos y contaminen el medio ambiente. ABSTRACT Developed societies generate a lot of waste, which need proper management. Thus, this problem requires increased attention from the society, due to the need to protect the environment. In this regard, efforts are focused on to minimize the generation of waste and find ways of taking advantage of those who are inevitable, much more advisable solutions from the technical, ecological and economic viewpoint to disposal or destruction. Industries should adopt precise measures to promote waste reduction, develop clean technologies that allow the saving of natural resources that we possess, and above all seek methods of reuse, recycling, recovery and valorisation of the waste generated in their production. The industry of the construction is a very receptive field for the development of new materials in which to incorporate these residues. The incorporation of different industrial residues in ceramic counterfoils appears as a cheap route to fix the different metallic present species in transformation of ornamental rocks, muds of galvanization or metallurgical, etc. In all the cases, the addition of these residues needs his previous characterization and the optimization of the conditions of conformed and of baking in case of his incorporation to the baked clay. Residues incorporated into construction materials include aluminium slag. The metallurgical industry produces during their fusion processes different types of slags. Recycling is one of the lines of interest to these industries. In the case of aluminium slag, their initial treatment consists of a recovery of the aluminium using mechanical methods followed by chemical treatment, or plasma. This method leads to that final slag just contains aluminium and is rich in soluble salts which limits storage in dumps. The slag is a mixture of aluminium metal and non-metallic such as oxides, nitrides and carbides of aluminium salts products and other metal oxides. The present Doctoral thesis has analysed the technical viability of the incorporation of aluminium slag from secondary Metallurgy in an array of baked clay. So they have been applied different treatments to the slag and have been applied different variables in its processing as the temperature of sintering, in addition to the content of slag or energy grinding. Its compaction with water between 5-10%, drying and sintering allows rectangular pieces of different size. From the point of view of the content of the slag, it is incorporated between 10 and 40% slag TT, that is to say, submitted a calcination prior to 750 ° C in air. The best results achieved correspond to 20% ESC TT, sintered at 980 ° C, as high levels of slag in accordance to pieces with black heart. The products obtained with the addition of 20% of slag from aluminium to clay, present a low expansion after sintering, better physical properties and mechanical, and higher thermal conductivity than the products obtained with clay, without addictions. Its density increases, decreases its absorption and increases its resistance to bending and compression, introducing a closed porosity and slag-matrix interaction. In all cases there is a superficial exudation of metallic aluminium, whose volume is related to the amount of slag added. By incorporating this content of slag, following a treatment of salt solution and subsequent calcination (ESC TTQ), are improved the properties of composite material not only on the calcined slag (ESC TT), but also in the slag without treatment (ESC). If the addition of 20% of slag added, is also treated, not only thermally but also chemically (ESC TTQ), they further improve the properties of the composite material, the product is more compact, less porous, so the values are higher density, minors are absorptions and greater resistance in bending and compression, to the products obtained with the addition of slag only treated thermally. Reaching values of compressive resistance characteristic of the order of 109 MPa. The thermal conductivity values obtained are also higher. Testing technology with pieces of 160 x 30 x 5 mm and optimized composite material of clay 20% ESCTTQ, consisted in the determination of its expansion by moisture, efflorescence and frost resistance, in general, showing a better performance than the clay without additions. Thus, we have obtained new ceramic matrix composite materials for construction, improving its physical, mechanical and thermal properties, using aluminium slag secondary metallurgy, as an option Valuation of these wastes, thus preventing them from being poured to landfills and pollute environment.