3 resultados para Wood furniture
em Instituto Politécnico de Viseu
Resumo:
This work intended to give a perspective of industrial wood protection in Portugal. A survey was made of the companies treating wood mainly for use classes 3 and 4 such as autoclave treatments with biocides and wood modification procedures. Currently there are 23 companies with 33 production plants with an autoclave installed for wood preservation by impregnation. There are also two companies producing modified wood by thermal treatment. Most of the plants are located in the central and northern regions of Portugal. The leading preservation chemicals used in Portugal are Tanalith E and Celcure brands. The main wood species used in all companies is Pinus pinaster from local producers. The products commercialized by the treating companies are diverse: pre-fabricated houses, garden furniture and playgrounds, decks, poles, stakes, and sawn wood. Modified wood producers sell mostly decks and cladding. Considerable changes are expected in the next few years due to the requirements of European Directives and the typical constraints of the Portuguese market.
Resumo:
Paraffin has been used as surface protection of wood throughout the ages but its use for impregnation to improve wood resistance to biodegradation is recent. This study determined the main improvements on wood properties with paraffin impregnation. Healthy Pinus pinaster Ait. wood was impregnated with paraffin at different levels using a hot–cold process. Weight gain, equilibrium moisture content and dimensional stability (ASE) at 35 and 65 % relative humidity, termite durability against Reticulitermes grassei (Clément), bending strength, bending stiffness (MOE) and Janka hardness were determined. Density increased from 0.57 to 0.99, ASE ranged between 38–96 % and 16–71 % for 35 and 65 % relative humidity, respectively. Equilibrium moisture content decreased from 9.9 and 12.0 % to 0.8 and 3.6 % for 35 and 65 % relative humidity. Termite durability improved from level 4 to level 3 of attack, and higher termite mortality was found in treated wood (52 % against 17 %). Bending strength (MOR) increased with paraffin weight gain, reaching a 39 % increase. MOE also increased by about 13 % for wood with a weight gain around 80 %. Janka hardness increased significantly reaching about 40 % for wood with 80 % weight gain. Paraffin impregnated wood has improved properties with regard to equilibrium moisture content, dimensional stability and density, bending strength and Janka hardness, and resistance against termites.
Resumo:
The aim of present work was to investigate the phenolic and volatile composition of cherry, acacia, and oak (from different species) wood chips. By the use of HPLC-DAD 18 different phenolic compounds were detected and quantified while for volatile composition, 33 different compounds were detected by GC-MS. In general, wood samples from oak species showed the higher number of phenolic compounds detected, while cherry wood samples showed the lowest levels. In addition, some individual phenolic compounds were detected, specifically in some wood samples, such as robinetin in acacia woods and naringenin in cherry wood. For volatile composition, cherry wood chips samples showed the lowest volatile composition followed by increasing order by acacia, French, Portuguese and American wood chip samples. Oak wood chip samples from American species showed the highest volatile content, as a result of high levels of several specific compounds (furfural, 5-methyfurfural, β-methyl-γ-octalactones, guaiacol, vanillin and siringaldehyde).