Silica final lenses under HiPER laser fusion reactor operation conditions


Autoria(s): Garoz Gómez, David; Rivera de Mena, Antonio; Juarez Mañas, Rafael; Alvarez Ruiz, Jesus; Gonzalez Arrabal, Raquel; Perlado Martin, Jose Manuel
Data(s)

2011

Resumo

We have studied the thermo-mechanical response and atomistic degradation of final lenses in HiPER project. Final silica lenses are squares of 75 × 75 cm2 with a thickness of 5 cm. There are two scenarios where lenses are located at 8 m from the centre: •HiPER 4a, bunches of 100 shots (maximum 5 DT shots <48 MJ at ≈0.1 Hz). No blanket in chamber geometry. •HiPER 4b, continuous mode with shots ≈50 MJ at 10 Hz to generate 0.5 GW. Liquid metal blanket in chamber design.

Formato

application/pdf

Identificador

http://oa.upm.es/11760/

Idioma(s)

spa

Publicador

E.T.S.I. Industriales (UPM)

Relação

http://oa.upm.es/11760/1/INVE_MEM_2011_103295.pdf

http://www.ifsa11.org/

info:eu-repo/semantics/altIdentifier/doi/null

Direitos

http://creativecommons.org/licenses/by-nc-nd/3.0/es/

info:eu-repo/semantics/openAccess

Fonte

proceedings of 7th International conference on inertial fusion sciences and applications, IFSA 2011 | 7th International conference on inertial fusion sciences and applications, IFSA 2011 | 12/09/2011 - 16/09/2011 | Bordeaux, Francia

Palavras-Chave #Energía Nuclear #Física
Tipo

info:eu-repo/semantics/conferenceObject

Ponencia en Congreso o Jornada

PeerReviewed