Thallium Bromide Deposited Using Spray Coating
Contribuinte(s) |
UNIVERSIDADE DE SÃO PAULO |
---|---|
Data(s) |
22/08/2013
22/08/2013
2012
|
Resumo |
Spray coating was used to produce thallium bromide samples on glass substrates. The influence of several fabrication parameters on the final structural properties of the samples was investigated. Substrate position, substrate temperature, solution concentration, carrying gas, and solution flow were varied systematically, the physical deposition mechanism involved in each case being discussed. Total deposition time of about 3.5 h can lead to 62-mu m-thick films, comprising completely packed micrometer-sized crystalline grains. X-ray diffraction and scanning electron microscopy were used to characterize the samples. On the basis of the experimental data, the optimum fabrication conditions were identified. The technique offers an alternative method for fast, cheap fabrication of large-area devices for the detection of high-energy radiation, i.e., X-rays and gamma-rays, in medical imaging. CAPES CAPES FAPESP FAPESP CNPq CNPq |
Identificador |
BRAZILIAN JOURNAL OF PHYSICS, NEW YORK, v. 42, n. 41367, supl. 1, Part 1, pp. 186-191, AUG, 2012 0103-9733 http://www.producao.usp.br/handle/BDPI/32680 10.1007/s13538-012-0073-2 |
Idioma(s) |
eng |
Publicador |
SPRINGER NEW YORK |
Relação |
BRAZILIAN JOURNAL OF PHYSICS |
Direitos |
closedAccess Copyright SPRINGER |
Palavras-Chave | #TLBR #THALLIUM BROMIDE #FILM #SPRAY COATING #SEMICONDUCTOR #RADIATION DETECTOR #RADIATION DETECTOR APPLICATIONS #GAMMA-RAY SPECTROSCOPY #X-RAY #TLBR FILMS #THIN-FILMS #TEMPERATURE #CRYSTALS #PURIFICATION #PYROLYSIS #CDZNTE #PHYSICS, MULTIDISCIPLINARY |
Tipo |
article original article publishedVersion |