Electrophoretic deposition of (Zn, Nb)SnO2-films varistor superficially modified with Cr3+
Contribuinte(s) |
Universidade Estadual Paulista (UNESP) |
---|---|
Data(s) |
21/10/2015
21/10/2015
01/07/2015
|
Resumo |
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq) Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP) Processo FAPESP: 2013/07296-2 Recently, there has been an important rise in the research and development aimed to improve the properties of SnO2-based varistors. Meanwhile, due to fact that ZnO-based varistors possess better electrical properties compared to SnO2-based varistors, it is shown that it is needful to add additives to improve their properties. In our study, the SnO2-powder was prepared by the chemical route (Pechini method) with addition of ZnO (1 mol%) and Nb2O5 (0.05 mol%). Films were obtained by the electrophoretic deposition of SnO2-based powder, following by microwave oven sintering. Cr3+ was deposited by EPD on the films surface and thermal treatment was carried out in a microwave oven. After electrical characterization the films showed nonlinear coefficient over 10, breakdown voltage around 60 V, low leakage current (approximate to 10(-6) A) and resistance over 200 kg cm. This indicates the efficiency of the used techniques to prepare varistor films with improved electrical properties after Cr3+ diffusion. (C) 2015 Elsevier Ltd. All rights reserved. |
Formato |
2083-2089 |
Identificador |
http://www.sciencedirect.com/science/article/pii/S0955221915000254 Journal Of The European Ceramic Society, v. 35, n. 7, p. 2083-2089, 2015. 0955-2219 http://hdl.handle.net/11449/129081 http://dx.doi.org/10.1016/j.jeurceramsoc.2015.01.022 WOS:000351794300011 |
Idioma(s) |
eng |
Publicador |
Elsevier B.V. |
Relação |
Journal Of The European Ceramic Society |
Direitos |
closedAccess |
Palavras-Chave | #SnO2 varistor #Pechini #Electrophoretic deposition #Microwave sintering #Cr3+ diffusion |
Tipo |
info:eu-repo/semantics/article |