Multidoped nanosized ceria powders were prepared by either modified glycine nitrate procedure (MGNP) or self-propagating reaction at room temperature (SPRT). As the dopants to CeO2, trivalent rare earth oxides such as Nd2O3, Sm2O3, Gd2O3, Dy2O3 and Y2O3 were used, with the total molar fraction of 20%. The pressed powder pellets were subjected to the densification by sintering at 1500 degrees C, in an air atmosphere. A single-phase crystalline form was evidenced by X-ray diffractometry for both sintered materials. By means of complex impedance measurements, the conductivity of the sintered samples was determined as a function of temperature. At 700 degrees C, the conductivity amounted to 2.19 x 10(-2) and 1.40 x 10(-2) ohm(-1) cm(-1) for the SPRT and for the MGNP sample, respectively. The corresponding values of activation energies of conductivity amounted to 0.72 (MGNP) and 0.59 (SPRT) eV in the temperature range 550-700 degrees C. (C) 2014 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Formato

9285-9292

Identificador

http://dx.doi.org/10.1016/j.ceramint.2014.01.151

Ceramics International. Oxford: Elsevier Sci Ltd, v. 40, n. 7, p. 9285-9292, 2014.

0272-8842

http://hdl.handle.net/11449/111415

10.1016/j.ceramint.2014.01.151

WOS:000337015200044

Idioma(s)

eng

Publicador

Elsevier B.V.

Relação

Ceramics International

Direitos

closedAccess

Palavras-Chave #Sintering #Ionic conductivity #CeO2 #Fuel cells
Tipo

info:eu-repo/semantics/article