Effect of ceramic surface treatment on the shear bond strength of a resin cement to different ceramic systems


Autoria(s): Ribeiro, Joao Gustavo Rabelo; Segalla, José Claudio Martins; Perez, Fabiano; Ribeiro, Jose Carlos Rabelo; Moyses, Marcos Ribeiro
Contribuinte(s)

Universidade Estadual Paulista (UNESP)

Data(s)

27/05/2014

27/05/2014

01/09/2012

Resumo

This study evaluated three surface treatments and their effects on the shear bond strength between a resin cement and one of three ceramics. The ceramic surfaces were evaluated with scanning electron microscopy (SEM ) as well. Specimens were treated with 50 μm aluminum oxide airborne particles, 10% hydrofluoric acid etching, or a combination of the two. Using a matrix with a center hole (5.0 mm × 3.0 mm), the ceramic bonding areas were filled with resin cement following treatment. The specimens were submitted to thermal cycling (1,000 cycles) and the shear bond strength was tested (0.5 mm/minute). The failure mode and the effect of surface treatment were analyzed under SEM . Data were submitted to ANOVA and a Tukey test (α = 0.05). Duceram Plus and IPS Empress 2 composite specimens produced similar shear bond strength results (p > 0.05), regardless of the treatment method used. Hydrofluoric acid decreased the shear bond strength of In-Ceram Alumina specimens. For all materials, surface treatments changed the morphological surface. All treatments influenced the shear bond strength and failure mode of the ceramic/resin cement composites.

Identificador

http://www.ncbi.nlm.nih.gov/pubmed/23032240

General Dentistry, v. 60, n. 5, 2012.

0363-6771

http://hdl.handle.net/11449/73554

2-s2.0-84866876268

Idioma(s)

eng

Relação

General Dentistry

Direitos

closedAccess

Tipo

info:eu-repo/semantics/article