Resumo

This study compared the bond strength durability of a feldspathic veneering ceramic to glass-infiltrated reinforced ceramics in dry and aged conditions. Disc shaped (thickness: 4 mm, diameter: 4 mm) of glass-infiltrated alumina (In-Ceram Alumina) and glass-infiltrated alumina reinforced by zirconia (In-Ceram Zirconia) core ceramic specimens (N=48, N=12 per groups) were constructed according to the manufacturers' recommendations. Veneering ceramic (VITA VM7) was fired onto the core ceramics using a mold. The core-veneering ceramic assemblies were randomly divided into two conditions and tested either immediately after specimen preparation (Dry) or following 30000 thermocycling (5-55 oC±1; dwell time: 30 seconds). Shear bond strength test was performed in a universal testing machine (cross-head speed: 1 mm/min). Failure modes were analyzed using optical microscope (x20). The bond strength data (MPa) were analyzed using ANOVA (α=0.05). Thermocycling did not decrease the bond strength results for both In-Ceram Alumina (30.6±8.2 MPa; P=0.2053) and In-Ceram zirconia (32.6±9 MPa; P=0.3987) core ceramic-feldspathic veneering ceramic combinations when compared to non-aged conditions (28.1±6.4 MPa, 29.7±7.3 MPa, respectively). There were also no significant differences between adhesion of the veneering ceramic to either In-Ceram Alumina or In-Ceram Zirconia ceramics (P=0.3289). Failure types were predominantly a mixture of adhesive failure between the veneering and the core ceramic together with cohesive fracture of the veneering ceramic. Long-term thermocycling aging conditions did not impair the adhesion of the veneering ceramic to the glass-infiltrated alumina core ceramics tested.

Formato

393-399

Identificador

http://www.minervamedica.it/en/journals/minerva-stomatologica/article.php?cod=R18Y2010N07A0393

Minerva stomatologica, v. 59, n. 7-8, p. 393-399, 2010.

0026-4970

http://hdl.handle.net/11449/71770

2-s2.0-79952798721

Idioma(s)

eng

Relação

Minerva stomatologica

Direitos

closedAccess

Palavras-Chave #glass #In Ceram Alumina #In Ceram Zirconia #In-Ceram Alumina #In-Ceram Zirconia #VITA VM7 #ceramics #comparative study #dental bonding #denture #equipment #evaluation #heat #humidity #in vitro study #materials testing #randomization #shear strength #time #tooth prosthesis #Ceramics #Dental Bonding #Dental Porcelain #Dental Veneers #Equipment Failure #Glass #Hot Temperature #Humidity #Materials Testing #Random Allocation #Shear Strength #Time Factors
Tipo

info:eu-repo/semantics/article