In vitro surface roughness of different glass ionomer cements indicated for ART restorations


Autoria(s): Momesso, Marília Gabriela Corrêa; da Silva, Renata Cristiane; Imparato, José Carlos Pettorossi; Molina, Celso; Navarro, Ricardo Scarparo; Ribeiro, Sidney José Lima
Contribuinte(s)

Universidade Estadual Paulista (UNESP)

Data(s)

27/05/2014

27/05/2014

01/04/2010

Resumo

Aim: The aim of this in vitro study was to evaluate the surface roughness of three glass ionomer cements (GICs) indicated for ART restorations. Methods: Ten cylindrical specimens of three commercial glass ionomers cements (Vidrion R - S.S. White, Maxxion R - FGM and Vitromolar DFL) were prepared (n=30) without surface finishing or protection. Twenty-four hours after preparation, the surface roughness measurements were obtained as the mean of three readings of the surface of each specimen by profilometry. The roughness values (Ra, μm) were subjected to one-way ANOVA and Tukey's test (p<0.05). Results: No statistically significant differences were observed between Vidrion R (0.18 ± 0.05) and Vitromolar (0.21 ± 0.05), whereas Maxxion R presented significantly higher roughness values than those of the other materials. Conclusions: It may be concluded that characteristics of particle size and composition of the different GICs affected their surface roughness 24 h after preparation.

Formato

77-80

Identificador

http://www.bibliotecadigital.unicamp.br/document/?code=43874

Brazilian Journal of Oral Sciences, v. 9, n. 2, p. 77-80, 2010.

1677-3217

1677-3225

http://hdl.handle.net/11449/71641

2-s2.0-77956988282

2-s2.0-77956988282.pdf

Idioma(s)

eng

Relação

Brazilian Journal of Oral Sciences

Direitos

openAccess

Palavras-Chave #ART #Glass ionomer cements #Profilometry #Restorative dental materials #Roughness