PMN powder samples with PbO excess of 0, 1,2 and 3% were submitted to the pressing and sintering at 1200°C for 4h with a heating rate of 3°C/min. A new sintering system, developed at our laboratories, was used. It allows obtaining more information on the sintering process. The sintered samples in the new system were compared to sintered samples in the C system. The microstructure, dielectric properties and the effect of the PbO excess in different sintering systems were compared. The N system permitted to obtain a ceramic with better properties, such density, dielectric constant and very homogeneous microstructure. |
Formato |
597-602 |
Identificador |
http://dx.doi.org/10.4028/www.scientific.net/MSF.416-418.597 Materials Science Forum, v. 416-418, n. 1, p. 597-602, 2003. 0255-5476 http://hdl.handle.net/11449/67234 10.4028/www.scientific.net/MSF.416-418.597 WOS:000182605200098 2-s2.0-0037282789 |
Idioma(s) |
eng |
Relação |
Materials Science Forum |
Direitos |
closedAccess |
Palavras-Chave | #Ceramics #Dielectrics #Microstructure #PMN #Sintering #Lead magnesium niobate #Lead oxide #Pyrochlore phase ratio #Composition effects #Crystal microstructure #Density (specific gravity) #Heating #Permittivity #Perovskite #Pressing (forming) #Lead compounds |
Tipo |
info:eu-repo/semantics/article |