Formation of colloidal particles of hydrous iron oxide by forced hydrolysis


Autoria(s): Meyer, Wagner R.; Pulcinelli, Sandra Helena; Santilli, Celso Valentim; Craievich, Aldo F.
Contribuinte(s)

Universidade Estadual Paulista (UNESP)

Data(s)

27/05/2014

27/05/2014

01/08/2000

Resumo

The mechanism of formation and growth of hydrous iron oxide (FeOOH) during the initial stages of forced hydrolyses of ferric chloride aqueous solution was studied by small angle X-ray scattering (SAXS). The effect of the hydrolysis temperature (60°C, 70°C and 80°C) and of the addition of urea on the formation of colloidal particles under isothermal conditions were investigated. Based on the experimental scattering functions in the Guinier range, we suggest the presence of elongated colloidal particles. The particle diameter and length, and their variation with time, were determined by fitting the form factor of prolate ellipsoids to the experimental scattering functions. We have assumed that our solutions are in a dilute state and that all colloidal particles are approximately of the same size. The colloidal particles have geometrical shapes similar to those of the subcrystals that build up the superstructure of β-FeOOH crystals, indicating that the formation of this hydrous iron oxide is governed by an aggregation process. Otherwise, the addition of urea hinders the growth and yields smaller particles, with a reduction in size greater than 50%. © 2000 Elsevier Science B.V. All rights reserved.

Formato

41-47

Identificador

http://dx.doi.org/10.1016/S0022-3093(00)00142-3

Journal of Non-Crystalline Solids, v. 273, n. 1-3, p. 41-47, 2000.

0022-3093

http://hdl.handle.net/11449/66204

10.1016/S0022-3093(00)00142-3

WOS:000088585700008

2-s2.0-0038631352

Idioma(s)

eng

Relação

Journal of Non-Crystalline Solids

Direitos

closedAccess

Tipo

info:eu-repo/semantics/article