The AlMCM-41 material with Si/Al=50 was synthesized by hydrothermal method, using cethyltrimethylammonium as template. The protonic H-AlMCM-41 acid form was obtained by ion exchange with ammonium chloride solution and subsequent calcination. The characterization of the material by several techniques showed that a good-quality MCM-41 material was obtained. High-density polyethylene (HDPE) has been submitted to thermal degradation alone, and in presence of the exchanged H-AlMCM-41 catalyst at a concentration of 1: 1 in mass (H-AlMCM-41/HDPE). The reactor was connected on line to a gas chromatograph connected to a mass spectrometer. This process was evaluated by thermogravimetry (TG), from 350 to 600degreesC, under helium dynamic atmosphere, with heating rates of 5.0; 10.0 and 20.0 degreesC/min. From TG curves, the activation energy, calculated using a multiple heating rate integral kinetic method, decreased from 225.5 KJ.mol(-1), for the pure polymer (HDPE), to 184.7 KJ.mol(-1), in the presence of the catalyst (H-AlMCM-41/HDPE).

Formato

473-478

Identificador

http://dx.doi.org/10.1016/S0167-2991(02)80578-X

Nanoporous Materials Iii. Amsterdam: Elsevier B.V., v. 141, p. 473-478, 2002.

0167-2991

http://hdl.handle.net/11449/36991

10.1016/S0167-2991(02)80578-X

WOS:000180926800059

Idioma(s)

eng

Publicador

Elsevier B.V.

Relação

Nanoporous Materials Iii

Direitos

closedAccess

Tipo

info:eu-repo/semantics/article