Microstructure and electric properties of a SnO2 based varistor
Contribuinte(s) |
Universidade Estadual Paulista (UNESP) |
---|---|
Data(s) |
20/05/2014
20/05/2014
01/01/1999
|
Resumo |
High non-linear J x E electrical characteristic (alpha=41) were obtained in the Nb2O5 and Cr2O3 doped CoO highly densified SnO2 ceramics. X-ray diffraction analysis showed that these ceramics are apparently single phase. Electrical properties and microstructure are highly dependent on the Cr2O3 concentration and on the sintering temperature. Excess of Cr2O3 leads to porous ceramics destroying the material's electrical characteristics probably due to precipitation of second phase of CoCr2O4 Dopant segregation and/or solid solution formation at the grain boundaries can be responsible for the formation of the electrical barriers which originate the varistor behaviour. (C) 1998 Elsevier B.V. Limited and Techna S.r.l. All rights reserved. |
Formato |
1-6 |
Identificador |
http://dx.doi.org/10.1016/S0272-8842(97)00076-X Ceramics International. Oxford: Elsevier B.V., v. 25, n. 1, p. 1-6, 1999. 0272-8842 http://hdl.handle.net/11449/36572 10.1016/S0272-8842(97)00076-X WOS:000077927800001 |
Idioma(s) |
eng |
Publicador |
Elsevier B.V. |
Relação |
Ceramics International |
Direitos |
closedAccess |
Tipo |
info:eu-repo/semantics/article |