Ultra-fine powders of Na1-xLixNbO3 (x=0; 0.06; 0.09; 0.12) were synthesized by the Polymeric Precursors Method. Such powders had their orthorhombic structures determined by X-ray diffraction and their surface area determined by BET isotherms (less than 10 m(2) g(-1)). Densification was followed by dilatometric study. The powders, calcined at 700 degrees C for 5 h, were sintered at 1290 degrees C during 2 h under ambient atmosphere with no application of extra pressure. The samples with relative densities higher than 95% were analyzed by impedance spectroscopy at room temperature, under a signal amplitude of 1 V-rms. Dielectric constants of about 180 and dielectric loss factor of about 0.03 were measured showing small dependence with frequency. The electrical properties were similar to those obtained for samples sintered by hot pressing. (C) 1999 Elsevier B.V. Limited and Techna S.r.l. All rights reserved.

Formato

455-460

Identificador

http://dx.doi.org/10.1016/S0272-8842(98)00054-6

Ceramics International. Oxford: Elsevier B.V., v. 25, n. 5, p. 455-460, 1999.

0272-8842

http://hdl.handle.net/11449/36481

10.1016/S0272-8842(98)00054-6

WOS:000081144900008

Idioma(s)

eng

Publicador

Elsevier B.V.

Relação

Ceramics International

Direitos

closedAccess

Palavras-Chave #sodium and lithium niobate #polymeric precursors #dielectric
Tipo

info:eu-repo/semantics/article