On the activation and physical degradation of boron-doped diamond surfaces brought on by cathodic pretreatments


Autoria(s): SALAZAR-BANDA, Giancarlo R.; CARVALHO, Adriana E. de; ANDRADE, Leonardo S.; ROCHA-FILHO, Romeu C.; AVACA, Luis A.
Contribuinte(s)

UNIVERSIDADE DE SÃO PAULO

Data(s)

20/10/2012

20/10/2012

2010

Resumo

The electrochemical activation and physical degradation of boron-doped diamond (BDD) electrodes with different boron doping levels after repeated cathodic pretreatments are reported. Galvanostatic cathodic pretreatment passing up to -14000 C cm(-2) in steps of -600 C cm(-2) using -1 A cm(-2) caused significant physical degradation of the BDD surface, with film detachment in some areas. Because of this degradation, a great increase in the electrochemically active area was observed in Tafel plots for the hydrogen evolution reaction (HER) in acid media. The minimum cathodic pretreatment needed for the electrochemical activation of the BDD electrodes without producing any observable physical degradation on the BDD surfaces was determined using electrochemical impedance spectroscopy (EIS) measurements and cyclic voltammetry: -9 C cm(-2), passed at -1 A cm(-2). This optimized cathodic pretreatment can be safely used when electrochemical experiments are carried out on BDD electrodes with doping levels in the range between 800 and 8000 ppm.

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

CNPq

CAPES

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

FAPESP

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Identificador

JOURNAL OF APPLIED ELECTROCHEMISTRY, v.40, n.10, p.1817-1827, 2010

0021-891X

http://producao.usp.br/handle/BDPI/31799

10.1007/s10800-010-0139-1

http://dx.doi.org/10.1007/s10800-010-0139-1

Idioma(s)

eng

Publicador

SPRINGER

Relação

Journal of Applied Electrochemistry

Direitos

restrictedAccess

Copyright SPRINGER

Palavras-Chave #Boron-doped diamond electrodes #Cathodic pretreatment #Surface erosion #Surface activation #Electrochemical impedance spectroscopy #WAVE VOLTAMMETRIC DETERMINATION #CHARGE-TRANSFER REACTIONS #DIFFERENT DOPING LEVELS #THIN-FILMS #ELECTROANALYTICAL DETERMINATION #SONOVOLTAMMETRIC DETERMINATION #ELECTROCHEMICAL-BEHAVIOR #CVD-DIAMOND #ELECTRODES #HYDROGEN #Electrochemistry
Tipo

article

original article

publishedVersion