Microstructure and magnetic properties of Ni50 Mn37 Sn13 Heusler alloy ribbons
Data(s) |
2008
|
---|---|
Resumo |
The Heusler alloy Ni50 Mn37 Sn13 was successfully produced as ribbon flakes of thickness around 7-10 μm melt spinning. Fracture cross section micrographs in the ribbon show the formation of a microcrystalline columnarlike microstructure, with their longer axes perpendicular to the ribbon plane. Phase transition temperatures of the martensite-austenite transformation were found to be MS =218 K, Mf =207 K, AS =224 K, and Af =232 K; the thermal hysteresis of the transformation is 15 K. Ferromagnetic L 21 bcc austenite phase shows a Curie point of 313 K, with cell parameter a=0.5971 (5) nm at 298 K, transforming into a modulated 7M orthorhombic martensite with a=0.6121 (7) nm, b=0.6058 (8) nm, and c=0.5660 (2) nm, at 150 K |
Formato |
application/pdf |
Identificador |
Santos, J.D., Sánchez, T., Álvarez, P., Sánchez, M.L., Llamazares, J.L.S., Hernándo, B., Escoda, Ll., Suñol, J.J. i Varga, R. (2008). Microstructure and magnetic properties of Ni50 Mn37 Sn13 Heusler alloy ribbons. Journal of Applied Physics, 103 (7), 07B326. Recuperat 7 febrer 2011, a http://link.aip.org/link/JAPIAU/v103/i7/p07B326/s1 0021-8979 (versió paper) 1089-7550 (versió electrònica) |
Idioma(s) |
eng |
Publicador |
American Institute of Physics |
Relação |
Reproducció digital del document publicat a: http://dx.doi.org/10.1063/1.2832330 © Journal of Applied Physics, 2008, vol. 103, núm. 7 Articles publicats (D-F) |
Direitos |
Tots els drets reservats |
Palavras-Chave | #Aliatges #Estany -- Propietats magnètiques #Manganès -- Propietats magnètiques #Microestructura #Níquel -- Propietats magnètiques #Alloys #Manganese -- Magnetic properties #Nickel -- Magnetic properties #Tin -- Magnetic properties #Microstructure |