Síntese do material mesoporoso MCM-41 usando esponja de água-doce como fonte de sílica


Autoria(s): Lacerda Júnior,Orivaldo da Silva; Cavalcanti,Rodrigo Marinho; Matos,Thaisa Moreira de; Venâncio,Jocilândia de Brito; Barros,Iuri Bezerra de; Veiga-Júnior,Valdir Florêncio da; Barros,Ivoneide de Carvalho Lopes
Data(s)

01/01/2013

Resumo

Fresh water sponge was used as a silica source for the synthesis of MCM-41 via the hydrothermal process. The silica was extracted from the sponge by washing with nitric acid and piranha solution. Synthesis of MCM-41 was performed at 100 °C for 5 days and the procedure was optimized, with modifications made to the leaching temperature of the silica and the synthesis of mesoporous material, which was characterized by XRD, FT-IR, SEM and adsorption of N2. The optimal result was achieved at a temperature of 135 °C for 3 days, showing ordered mesoporous material with a surface area of 1080 m² g-1.

Formato

text/html

Identificador

http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422013000900012

Idioma(s)

pt

Publicador

Sociedade Brasileira de Química

Fonte

Química Nova v.36 n.9 2013

Palavras-Chave #synthesis #bio-silica #mesoporous
Tipo

journal article