Recuperação de metais de catalisadores usados de hidrotratamento (NiMo E CoMo/AL2O3)


Autoria(s): Afonso,Júlio C.; Lajter,Karen; Góes,Ronny S.
Data(s)

01/08/1997

Resumo

This work presents a detailed study of the leaching behavior of deactivated hydrotreating catalysts (CoMo, NiMo/Al2O3) in presence of oxalate and NH4+ ions in various media. The yield of metals recovery may be optimized by adjusting several experimental parameters (time, temperature, etc). Leaching is limited by physical factors (diffusional effects caused by coke) and by the existence of silicate/spinel-like species which are poorly soluble in leaching solutions. Coke may be eliminated by an oxidation step at temperatures between 300-400ºC. Above 400ºC, solubilization of Ni and Co is drastically reduced. 50-90% wt of sulphate species and 15-30% wt of phosphate ions are solubilized during leaching. Silicon (as SiO2) is not solubilized. The best Ni-Co-Mo recoveries are in the 70-90% wt range; Fe recovery may be quantitative, whereas Al leaching may be lower than 5% wt.

Formato

text/html

Identificador

http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40421997000400002

Idioma(s)

pt

Publicador

Sociedade Brasileira de Química

Fonte

Química Nova v.20 n.4 1997

Palavras-Chave #spent catalyst #metals recovery #oxalate ions
Tipo

journal article