Preliminary Studies of Remedial Measures for the Prevention of Bridge Deck Deterioration, HR-146, 1970


Autoria(s): Desconhecido
Data(s)

01/03/1970

Resumo

Four series of five specimens each were investigated for static and fatigue strength. These four series differed in that there were two variables, the first being the subsidence of concrete around reinforcing bars and the second being shrinkage due to two different curing conditions. The combinations of these variables were then compared to each other by use of, load-deflection curves and S-H fatigue curves.

Formato

pdf

Identificador

http://publications.iowa.gov/22109/1/IADOT_HR_146_Preliminary_Prevention_Bridge_Deck_Deterioration_1970.pdf

(1970) Preliminary Studies of Remedial Measures for the Prevention of Bridge Deck Deterioration, HR-146, 1970. Transportation, Department of

Idioma(s)

en

Relação

http://publications.iowa.gov/22109/

Palavras-Chave #Transportation #Bridges and tunnels #Research #Concrete #Maintenance and preservation
Tipo

Departmental Report

NonPeerReviewed