COMPARISON OF THE BEHAVIOR OF CYCLIC AND LINEAR POLYSTYRENE IN DILUTE-SOLUTION


Autoria(s): ZHANG H; HE ZD
Data(s)

1991

Resumo

Using a low angle laser light scattering photometer, the second virial coefficients (A2) of both cyclic and linear polystyrene were determined in cyclohexane, toluene and methyl ethyl ketone (MEK) solutions. From the data obtained in cyclohexane solution the theta-temperature of cyclic polystyrene was determined to be 30-degrees-C. In toluene solution A2 of cyclic polystyrene is smaller than that of linear polystyrene with the same molecular weight, but in MEK the values are similar.

Identificador

http://202.98.16.49/handle/322003/38465

http://www.irgrid.ac.cn/handle/1471x/163606

Idioma(s)

英语

Fonte

ZHANG H;HE ZD.COMPARISON OF THE BEHAVIOR OF CYCLIC AND LINEAR POLYSTYRENE IN DILUTE-SOLUTION,POLYMER COMMUNICATIONS,1991,32(8):239-241