Crystallization and characterization of substoichiometric compound (W0.5Al0.5)C-0..5 obtained by solid-state reaction
Data(s) |
2006
|
---|---|
Resumo |
(W0.5Al0.5)C-0.5 substoichiometric compound is synthesized by a combination of mechanical milling and high-pressure reactive sintering. X-ray diffraction is used to monitor the phase changes and crystallization of (W0.5Al0.5) C-0.5 during the whole reaction process. As a result, (W0.5Al0.5) C-0.5 is identified as the hexagonal WC-type belonging to the P-6m2 space group (No. 187), and the lattice parameters of (W0.5Al0.5)C-0.5 are calculated to be a = 2.907 (1) angstrom, c = 2.838 (1) angstrom, which are very similar to those of WC even if there are approximately 50 pct carbon vacancies in the cell of (W0.5Al0.5)C-0.5 as compared with WC. The substoichiometric (W0.5Al0.5)C-0.5 compound has a Vickers microhardness of 2385 +/- 70 kg mm(-2), which is as high as that of WC, while its density is far lower than that of WC. |
Identificador | |
Idioma(s) |
英语 |
Fonte |
Yan JM;Ma XF;Zhao W;Tang HG;Zhu CJ;Cai SG .Crystallization and characterization of substoichiometric compound (W0.5Al0.5)C-0..5 obtained by solid-state reaction,METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,2006,37A(5):1692-1695 |
Tipo |
期刊论文 |