Synthesis, reactive mechanism and thermal stability of W1-xAlxC (x=0.33, 0.5, 0.75, 0.86) nanocrystalline


Autoria(s): Tang HG; Ma XF; Zhao W; Yan XW; Yan JM
Data(s)

2004

Resumo

W1-xAlxC (x = 0.33, 0.50, 0.75, 0.86) solid solutions have been synthesized directly by ball-milling tungsten powder, aluminum powder and activated carbon. The structural development of W0.5Al0.5C phase with the milling times up to 160 h has been followed using X-ray diffraction. X-ray photoelectron spectra demonstrate that Al atom takes the place of W. High temperature annealing experiment reveals that Al is stable in hexagonal structure to 1873 K. Transmission electron microscopy image shows that the grain size of the prepared powders is about 5 nm.

Identificador

http://ir.ciac.jl.cn/handle/322003/14759

http://www.irgrid.ac.cn/handle/1471x/150512

Idioma(s)

英语

Fonte

Tang HG;Ma XF;Zhao W;Yan XW;Yan JM.Synthesis, reactive mechanism and thermal stability of W1-xAlxC (x=0.33, 0.5, 0.75, 0.86) nanocrystalline,MATERIALS RESEARCH BULLETIN,2004,39(4-5):707-713

Tipo

期刊论文