Preparation of CeO2-ZrO2 ceramic fibers by electrospinning


Autoria(s): Zhang YF; Li JY; Li Q; Zhu L; Liu XD; Zhong XH; Meng J; Cao XQ
Data(s)

2007

Resumo

Electrospinning was employed to fabricate polymer-ceramic composite fibers from solutions containing poly(vinyl pyrrolidone) (PVP), Ce(NO3)(3)(.)6H(2)O and ZrOCl2-8H(2)O. Upon firing the composite fibers at 1000 degrees C, Ce(0.67)Zr(0.33)O(2)fibers with diameters ranging from 0.4 to 2 mu m were synthesized. These fibers exhibit strong resistance to sintering. They still have specific surface area around 11.8 m(2)/g after being heated at 1000 degrees C for 6 h.

Identificador

http://ir.ciac.jl.cn/handle/322003/14165

http://www.irgrid.ac.cn/handle/1471x/149924

Idioma(s)

英语

Fonte

Zhang YF;Li JY;Li Q;Zhu L;Liu XD;Zhong XH;Meng J;Cao XQ.Preparation of CeO2-ZrO2 ceramic fibers by electrospinning,JOURNAL OF COLLOID AND INTERFACE SCIENCE,2007 ,307(2):567-571

Palavras-Chave #OXYGEN STORAGE #CATALYSTS #STABILITY #SYSTEM
Tipo

期刊论文