High-pressure sintered yttria stabilized zirconia ceramics


Autoria(s): Li Q; Zhang YF; Ma XF; Meng J; Cao XQ
Data(s)

2009

Resumo

Fast densification of 8YSZ ceramics under a high pressure of 4.5 GPa was carried out at different temperatures (800, 1000, 1450 degrees C), by which a high relative density above 92% could be obtained. FT-Raman spectra indicate that the 8YSZ underwent a phase transition from partially tetragonal to partially cubic phase as temperatures increase from 1000 to 1450 degrees C when sintering under high pressure. The electrical properties of the samples under different high-pressure sintering conditions were measured by complex impedance method. The total conductivity of 0.92 x 10(-2) S cm(-1) at 800 degrees C has been obtained for 8YSZ under high pressure at 1450 degrees C, which is about 200 degrees C lower than that of the samples prepared by conventional pressureless sintering.

Identificador

http://202.98.16.49/handle/322003/11491

http://www.irgrid.ac.cn/handle/1471x/147984

Idioma(s)

英语

Fonte

Li Q;Zhang YF;Ma XF;Meng J;Cao XQ.High-pressure sintered yttria stabilized zirconia ceramics,CERAMICS INTERNATIONAL,2009,35(1):453-456

Palavras-Chave #IONIC-CONDUCTIVITY #DENSIFICATION #RAMAN #NANOCERAMICS
Tipo

期刊论文