Residual strength of hot pressed zirconium diboride (ZrB2) after exposure to high temperatures


Autoria(s): Patel, Manish; Reddy, JJ; Prasad, Bhanu VV; Subrahmanyam, J; Jayaram, Vikram
Data(s)

15/02/2012

Resumo

ZrB2 with different amounts of B4C additive (0-5 wt.%) has been hot pressed at 2000 degrees C and 25 MPa for 1 h. By addition of B4C, density as well as micro-hardness increased. For lower B4C content (0.5 and 1 wt.%), hot pressed ZrB2 shows considerable improvement in flexural strength after exposure in air at 1000 C for 5 h, while higher B4C content (3 and 5 wt.%) leads to marginal or no improvement. For any content of B4C, flexural strength after exposure in air at 1500 degrees C for 5 h is lower than as-hot pressed ZrB2. (C) 2011 Elsevier B.V. All rights reserved.

Formato

application/pdf

Identificador

http://eprints.iisc.ernet.in/44309/1/Residual.pdf

Patel, Manish and Reddy, JJ and Prasad, Bhanu VV and Subrahmanyam, J and Jayaram, Vikram (2012) Residual strength of hot pressed zirconium diboride (ZrB2) after exposure to high temperatures. In: Materials Science and Engineering: A, 535 . pp. 189-196.

Publicador

Elsevier Science

Relação

http://dx.doi.org/10.1016/j.msea.2011.12.062

http://eprints.iisc.ernet.in/44309/

Palavras-Chave #Materials Engineering (formerly Metallurgy)
Tipo

Journal Article

PeerReviewed