2 resultados para Retification®


Relevância:

10.00% 10.00%

Publicador:

Resumo:

The objective of this study was evaluate the effects of retification® temperatures and times on thickness variation from Eucalyptus grandis timber. Boards from logs of 30-year-old Eucalyptus grandis trees, from São Paulo Forest Institute in Santa Barbara, Brazil, were thermally modified at 180ºC for 2.5 hours, at 200ºC for 3.0 hours and 200ºC for 4.0 hours. The results showed that: (1) the thermally modified wood at 200°C by 3.0 to 4.0 hours showed increased thickness between 0.698 mm and 0.874 mm due to the internal cracks, (2) the thermally modified wood at 180°C by 2.5 hours has a decreased from 0,177 mm in thickness and the absences of internal cracks.