This PhD project has expanded the knowledge in the area of profluorescent nitroxides with regard to the synthesis and characterisations of novel profluorescent nitroxide probes as well as physical characterisation of the probe molecules in various polymer/physical environments. The synthesis of the first example of an azaphenalene-based fused aromatic nitroxide TMAO, [1,1,3,3-tetramethyl-2,3-dihydro-2-azaphenalen-2-yloxyl, was described. This novel nitroxide possesses some of the structural rigidity of the isoindoline class of nitroxides, as well as some properties akin to TEMPO nitroxides. Additionally, the integral aromatic ring imparts fluorescence that is switched on by radical scavenging reactions of the nitroxide, which makes it a sensitive probe for polymer degradation. In addition to the parent TMAO, 5 other azaphenalene derivatives were successfully synthesised. This new class of nitroxide was expected to have interesting redox properties when the structure was investigated by high-level ab initio molecular orbitals theory. This was expected to have implications with biological relevance as the calculated redox potentials for the azaphenalene ring class would make them potent antioxidant compounds. The redox potentials of 25 cyclic nitroxides from four different structural classes (pyrroline, piperidine, isoindoline and azaphenalene) were determined by cyclic voltammetry in acetonitrile. It was shown that potentials related to the one electron processes of the nitroxide were influenced by the type of ring system, ring substituents or groups surrounding the moiety. Favourable comparisons were found between theoretical and experimental potentials for pyrroline, piperidine and isoindoline ring classes. Substitution of these ring classes, were correctly calculated to have a small yet predictable effect on the potentials. The redox potentials of the azaphenalene ring class were underestimated by the calculations in all cases by at least a factor of two. This is believed to be due to another process influencing the redox potentials of the azaphenalene ring class which is not taken into account by the theoretical model. It was also possible to demonstrate the use of both azaphenalene and isoindoline nitroxides as additives for monitoring radical mediated damage that occurs in polypropylene as well as in more commercially relevant polyester resins. Polymer sample doped with nitroxide were exposed to both thermo-and photo-oxidative conditions with all nitroxides showing a protective effect. It was found that isoindoline nitroxides were able to indicate radical formation in polypropylene aged at elevated temperatures via fluorescence build-up. The azaphenalene nitroxide TMAO showed no such build-up of fluorescence. This was believed to be due to the more labile bond between the nitroxide and macromolecule and the protection may occur through a classical Denisov cycle, as is expected for commercially available HAS units. Finally, A new profluorescent dinitroxide, BTMIOA (9,10-bis(1,1,3,3- tetramethylisoindolin-2-yloxyl-5-yl)anthracene), was synthesised and shown to be a powerful probe for detecting changes during the initial stages of thermo-oxidative degradation of polypropylene. This probe, which contains a 9,10-diphenylanthracene core linked to two nitroxides, possesses strongly suppressed fluorescence due to quenching by the two nitroxide groups. This molecule also showed the greatest protective effect on thermo-oxidativly aged polypropylene. Most importantly, BTMIOA was found to be a valuable tool for imaging and mapping free-radical generation in polypropylene using fluorescence microscopy.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The increasing use of biodegradable devices in tissue engineering and regenerative medicine means it is essential to study and understand their degradation behaviour. Accelerated degradation systems aim to achieve similar degradation profiles within a shorter period of time, compared with standard conditions. However, these conditions only partially mimic the actual situation, and subsequent analyses and derived mechanisms must be treated with caution and should always be supported by actual long-term degradation data obtained under physiological conditions. Our studies revealed that polycaprolactone (PCL) and PCL-composite scaffolds degrade very differently under these different degradation conditions, whilst still undergoing hydrolysis. Molecular weight and mass loss results differ due to the different degradation pathways followed (surface degradation pathway for accelerated conditions and bulk degradation pathway for simulated physiological conditions). Crystallinity studies revealed similar patterns of recrystallization dynamics, and mechanical data indicated that the scaffolds retained their functional stability, in both instances, over the course of degradation. Ultimately, polymer degradation was shown to be chiefly governed by molecular weight, crystallinity susceptibility to hydrolysis and device architecture considerations whilst maintaining its thermodynamic equilibrium.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Emission spectroscopy was used to investigate ignition and combustion characteristics of supersonic combustion ramjet engines. Two-dimensional scramjet models with inlet injection, fuelled with hydrogen gas, were used in the study. The scramjet engines were configured to operate in radical farming mode, where combustion radicals are formed behind shock waves reflected at the walls. The chemiluminescence emission signals were recorded in a two-dimensional, time-integrated fashion to give information on the location and distribution of the radical farms in the combustors. High signal levels were detected in localised regions immediately downstream of shock reflections, an indication of localised hydroxyl formation supporting the concept of radical farming. Results are presented for a symmetric as well as an asymmetric scramjet geometry. These data represent the first successful visualisation of radical farms in the hot pockets of a supersonic combustor. Spectrally resolved measurements have been obtained in the ultraviolet wavelength range between 300 and 400 nm. This data shows that the OH! chemiluminescence signal around 306nm is not the most dominant source of radiation observed in the radical farms.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A correlation has been established between the heat of depolymerization (DeltaH) of vinyl polymers for going from solid polymer state to gaseous monomer state and the activation energy (E) of degradation. On this basis it has been shown that the rate controlling step in the degradation lies in the initiation step. Attempt has been made to correlate theE and DeltaH with glass transition temperature (Tg) and melting temperature (Tm) of the polymers.[/ p]

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Bioresorbable polymers such as PLA have an important role to play in the development of temporary implantable medical devices with significant benefits over traditional therapies. However, development of new devices is hindered by high manufacturing costs associated with difficulties in processing the material. A major problem is the lack of insight on material degradation during processing. In this work, a method of quantifying degradation of PLA using IR spectroscopy coupled with computational chemistry and chemometric modeling is examined. It is shown that the method can predict the quantity of degradation products in solid-state samples with reasonably good accuracy, indicating the potential to adapt the method to developing an on-line sensor for monitoring PLA degradation in real-time during processing.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

High density poly(ethylene) has been submitted to thermal degradation alone, and in the presence of silicoaluminophosphate SAPO-37. The processes were carried out in a reactor connected on line to a gas chromatograph/mass spectrometer in order to analyze the evolved products. Polymer degradation was also evaluated by thermogravimetry, from room temperature until 800 degreesC, under nitrogen dynamic atmosphere, with multiple heating rates. From TG curves, the activation energy related to degradation process was calculated using the Flynn and Wall multiple heating rate kinetic model for pure polymer (PE) and for polymer in the presence of catalyst (PE/S37). SAPO-37 showed good selectivity for low molecular mass hydrocarbons in PE catalytic degradation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The large use of plastics in the world generates a large amount of waste which persists around 200 years in the environment. To minimize this effect is important to search some new polymer materials: the blends of biodegradable polymers with synthetic polymers. It is a large area that needs an Intensive research to investigate the blends properties and its behavior face to the different treatments to aim at the blodegradation. The blends used In this work are: some blodegradable polymers such as: poly(hydroxybutyrate) (PHB) and poly(s-polycaprolactone) (PCL) with a synthetic polymer, polypropylene (PP), in lower concentration. These blends were prepared using an internal mixer (Torque Rheometer), and pressed. These films were submitted to fungus biotreatment. The films analyses will be carried out by Fourier Transform Infrared (FTIR), UV-Vis absorption (UV-Vis), Scanning Electronic Microscopy (SEM), DSC and TGA. © 2008 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This edition of Polymer Degradation and Stability is dedicated to papers which were presented in the session on ‘Chemical Modification’ at the Third International Conference on Modification Degradation and Stabilisation of Polymers (MoDeSt) held in Lyon in August 2004. This was the third meeting of the MoDeSt Society which was set up in the year 2000 under the chairmanship of Professor Franco LaMantia; the earlier meetings were held in Palermo (2000) and Budapest (2002). The overall goal of the MoDeSt Society is to promote the latest research carried out in University laboratories, in public organisations and in industry through publications, and organisation of biannual scientific conferences and workshops that act as forums for scientific developments and for promoting networking between academics and industrialists from across the field of polymer modification, degradation and stabilisation. In September 2004, Professor Norman Billingham was elected as Chairman of the Society. The conference was organised by Dr Alain Michel and Veronique Bounor-Legare of the University Claude Bernard, Lyon 1, attracting over 250 delegates with the ‘Chemical Modification’ Session alone enjoying 54 oral presentations and many more poster presentations. We are all very grateful to the organisers for running such a successful and enjoyable meeting. I wish to thank my co-editors, Professors Philippe Dubois and Domenico Acierno and Dr Alain Michel, for their cooperation in the editorial task of the papers published in this special issue. On behalf of the editors of this issue, I wish to express our appreciation to the Editor-in-Chief of Polymer Degradation and Stability, Professor Norman Billingham, for the support and help received during the preparation of this special issue.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Free-radical processes underpin the thermo-oxidative degradation of polyolefins. Thus, to extend the lifetime of these polymers, stabilizers are generally added during processing to scavenge the free radicals formed as the polymer degrades. Nitroxide radical precursors, such as hindered amine stabilizers (HAS),1,2 are common polypropylene additives as the nitroxide moiety is a potent scavenger of polymer alkyl radicals (R¥). Oxidation of HAS by radicals formed during polypropylene degradation yields nitroxide radicals (RRNO¥), which rapidly trap the polymer degradation species to produce alkoxyamines, thus retarding oxidative polymer degradation. This increase in polymer stability is demonstrated by a lengthening of the “induction period” of the polymer (the time prior to a sharp rise in the oxidation of the polymer). Instrumental techniques such as chemiluminescence or infrared spectroscopy are somewhat limited in detecting changes in the polymer during the initial stages of degradation. Therefore, other methods for observing polymer degradation have been sought as the useful life of a polymer does not extend far beyond its “induction period”

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A technique is described whereby micro-ATR/FTIR imaging can be used to follow polymer degradation reactions in situ in real time. The internal reflection element (IRE) assembly is removed from the ATR objective and polymer is solvent cast directly onto the IRE surface. The polymer is then subjected to degradation conditions and molecular structural changes monitored by periodically replacing the IRE assembly back in the ATR objective and collecting spectra which can be used to construct images. This approach has the benefit that the same part of the sample is always studied, and that contact by pressure which might damage the polymer surface is not required. The technique is demonstrated using the polymer Topas which was degraded by exposure to UVC light in air.