InAs self-organized nanostructures were grown with variant deposition thickness and growth rate on closely matched InAlAs/InP by molecular-beam epitaxy. The structural properties. of InAs and InAlAs layer were studied. It is found that the InAs morphology is insensitive to the growth conditions. Transmission electron microscopy and reflectance difference spectroscopy measurements show that the InAlAs matrix presents lateral composition modulation which gives birth to surface anisotropy. Based on the dependence of the InAs morphology on the anisotropy of the InAlAs layer, a modified Stranski-Krastanow growth mode is presented to describe the growth of the nanostructure on a composition-modulated surface.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The A1 compositional distribution of A1GaN is investigated by cathodoluminescence (CL). Monochromatic CL images and CL spectra reveal a lateral A1 compositional inhomogeneity, which corresponds to surface hexagonal patterns. Cross-sectional CL images show a relatively uniform Al compositional distribution in the growth direction, indicating columnar growth mode of A1GaN films. In addition, a thin A1GaN layer with lower Al composition is grown on top of the buffer A1N layer near the bottom of the A1GaN epilayer because of the larger lateral mobility of Ga adatoms on the growth surface and their accumulation at the grain boundaries.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have investigated the growth of AlGaN epilayers on a sapphire substrate by metalorganic chemical vapour deposition using various low-temperature ( LT) AlN buffer thicknesses. Combined scanning electron microscopy and cathodoluminescence investigations reveal the correlation between the surface morphology and optical properties of AlGaN films in a microscopic scale. It is found that the suitable thickness of the LT AlN buffer for high quality AlGaN growth is around 20 nm. The Al compositional inhomogeneity of the AlGaN epilayer is attributed to the low lateral mobility of Al adatoms on the growing surface.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The authors report the self-organized growth of InAs/InAlAs quantum wires on nominal (001) InP substrate and (001) InP substrates misoriented by 2 degrees, 4 degrees, and 8 degrees towards both [-110] and [110]. The influence of substrate misorientation on the structural and optical properties of these InAs/InAlAs quantum wires is studied by transmission electron microscopy and photoluminescence measurements. Compared with that grown on nominal (001) InP substrate, the density of InAs/InAlAs quantum wires grown on misoriented InP(001) substrates is enhanced. A strong lateral composition modulation effect take place in the InAlAs buffer layers grown on misoriented InP substrates with large off-cut angles (4 degrees and 8 degrees), which induces a nucleation template for the first-period InAs quantum wires and greatly improve the size distribution of InAs quantum wires. InAs/InAlAs quantum wires grown on InP (001) substrate 8 degrees off cut towards [-110] show the best size homogeneity and photoluminescence intensity. (c) 2007 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of Si and Mg doping on the crystalline quality and In distribution in the InGaN films were studied by atomic force microscope (AFM), triple crystal X-ray diffraction (TCXRD) and Rutherford backscattering spectrometry (RBS). The undoped, Si-doped and Mg-doped InGaN films were grown by metalorganic chemical vapor deposition (MOCVD) on (0 0 0 1) sapphire substrates. The electronic concentration in the Si-doped InGaN is about 2 x 10(19) cm(-3). It is found that the crystalline quality and In distribution in InGaN is slightly affected by the Si doping. In the Mg doped-case, the hole concentration is about 4 x 10(18) cm(-3) after annealing treatment. The surface morphology and crystalline quality of the Mg-doped InGaN are deteriorated significantly compared with the undoped InGaN. The growth rate of Mg-doped InGaN is higher than the undoped InGaN. Mg doping enhances the In incorporation in the InGaN alloy. The increase in In composition in the growth direction is more severe than the undoped InGaN. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High-quality AlInGaN quaternary layers were grown on c-Al2O3 using a thick GaN template. A full width at half maximum of 0.075 degrees from AlInGaN(0004) rocking curve and a minimum yield of 5.6% from Rutherford backscattering/channelling spectrometry (RBS) prove the AlInGaN layer of a comparable crystalline quality with GaN layers. The chemical compositions (both of Al and In contents) of AlInGaN layers are directly obtained from RBS and elastic recoil detection analysis. The lattice parameters both in perpendicular and parallel directions are deduced from X-ray diffraction. The AlInGaN layer is found to process a compressive strain in parallel direction and a tensile strain in perpendicular direction. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To fabricate nitride-based ultraviolet optoelectronic devices, a deposition process for high-Al-composition AlGaN (Al content > 50%) films with reduced dislocation densities must be developed. This paper describes the growth of high-Al-composition AlGaN film on (0001) sapphire via a LT AIN nucleation layer by low pressure metalorganic chemical vapor deposition (LPMOCVD). The influence of the low temperature AIN buffer layer thickness on the high-Al-content AlGaN epilayer is investigated by triple-axis X-ray diffraction (TAXRD), scanning electron microscopy (SEM), and optical transmittance. The results show that the buffer thickness is a key parameter that affects the quality of the AlGaN epilayer. An appropriate thickness results in the best structural properties and surface morphology. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It is important to acquire the composition of Si1-xGex layer, especially that with high Ge content, epitaxied on Si substrate. Two nondestructive examination methods, double crystals X-ray diffraction (DCXRD) and micro-Raman measurement, were introduced comparatively to determine x value in Si1-xGex: layer, which show that while the two methods are consistent with each other when x is low, the results obtained from double crystals X-ray diffraction are not credible due to the large strain relaxation occurring in Si1-xGex layers when Ge content is higher than about 20%. Micro-Raman measurement is more appropriate for determining high Ge content than DCXRD.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structural and optical properties of GaAsSb/GaAs quantum wells (QWs) and strain-compensated GaAsP/GaAs/GaAsSb/GaAs/GaAsP QWs grown on a GaAs substrate by molecular beam epitaxy are investigated using high-resolution x-ray diffraction and photoluminescence (PL) measurements. We demonstrated that the insertion of tensile GaAsP layers into the active region of GaAsSb/GaAs QWs effectively improves the structural and optical quality. Even the Sb composition is as high as 0.39. The PL spectra at 11 K and room temperature indicate that the PL peak of strain-compensated QWs has a narrower linewidth and higher intensity in comparison to the sample without strain compensation. The results of PL peak blueshift with increasing excitation show the strain-compensated GaAsSb/GaAs interface characteristic of type-I band alignment. (C) 2003 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

GaN1-xPx ternary alloys with high P compositions were deposited on sapphire substrates by means of metal-organic chemical vapor deposition. Depth profiles of the elements indicate that the maximum P/N composition ratio is about 17% and a uniform distribution of the P atoms in the alloys is achieved. 2theta/omega XRD spectra demonstrate that the (0002) peak of the GaN1-xPx alloys shifts to smaller angle with increasing P composition. From the photoluminescence (PL) spectra, the red shifts to the bandedge emission of GaN are determined to be 73, 78, 100 and 87 meV for the GaN1-xPx alloys with the P/N composition ratios of 3%, 11%, 15% and 17%, respectively. No PL peak related to GaP is observed, indicating that the phase separation between GaN and GaP is well suppressed in our GaN1-xPx samples. (C) 2003 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

InxGa1-xAs self-organized quantum dots with x=1.0, 0.5, and 0.35 have been grown by molecular beam epitaxy. The areal density, distribution, and shapes have been found to be dependent on x. The dot shape changes from a round shape for x=1.0 to an elliptical shape for x less than or equal to 0.5. The major axis and minor axis of the elliptical InxGa1-xAs dots are along the [(1) over bar 10] and [110] directions, respectively. The ordering phenomenon is also discussed. It is suggested that the dot-dot interaction may play important roles in the self-organization process. (C) 2000 American Institute of Physics. [S0021-8979(00)10701-7].

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The deposition of InxGa1-xAs (0.2 less than or equal to x less than or equal to 0.5) on (311)B GaAs surfaces using solid source molecular beam epitaxy (MBE) has been studied. Both AFM and photoluminescence emission showed that homogeneous quantum dots could be formed on (311)B GaAs surface when indium composition was around 0.4. Indium composition had a strong influence on the size uniformity and the lateral alignment of quantum dots. Compared with other surface orientation, (100) and (n11) A/B (n=1,2,3), photoluminescence measurement confirmed that (311)B surface is the most advantageous in fabricating uniform and dense quantum dots.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Self-assembled InxGa1-xAs quantum dots (QDs) on (311)A/B GaAs surfaces have been grown by molecular beam epitaxy (MBE). Spontaneously ordering alignment of InxGa1-xAs with lower In content around 0.3 have been observed. The direction of alignment orientation of the QDs formation differs from the direction of misorientation of the (311)B surface, and is strongly dependent upon the In content x. The ordering alignment become significantly deteriorated as the In content is increased to above 0.5 or as the QDs are formed on (100) or (311)A substrates. (C) 1999 Elsevier Science B.V. All rights reserved.