243 resultados para butadiene diepoxide


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The miscibilities of blends of homopolystyrene/styrene-butadiene/styrene (PS/SBS) and PS/SB-4A (4-arm star block copolymer) have been studied by dynamic mechanical analysis (DMA) and C-13 CPMAS NMR techniques. The results indicate that the miscibilities o

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The microstructures of styrene-butadiene triblock (SBS) and styrene-butadiene four-arm star block (SB-4A) copolymers and their blends with homopolystyrene (PS) of different molecular weights, MPS, have been investigated by means of small-angle X-ray scatt

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The proton spin-spin relaxation times (T-2(H)) at different temperatures (from 160 to 390 K) have been determined for polystyrene (PS) and four-arm star styrene-butadiene block copolymer (SB-4A) and its blends with PS of different molecular weights (M(PS)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Raw polymer and compound of hydrogenated acrylonitrile butadiene rubber (HNBR) were subjected to gamma-ray irradiation. Crosslinking was found to be the main chemical reaction induced by irradiation; the ratio of chain scission to crosslinking as well as

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(acrylonitrile-butadiene-styrene), polycarbonate (PC), and two types of antioxidants have been blended by an extruder twin screw. Notched Izod impact strength, tensile property, and melting flow index (MFI) were measured for the blends including diffe

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polycarbonate (PC) and poly(acrylonitrile-butadiene-styrene) (ABS) was co-extruded at different weight ratios by a single screw extruder. In order to obtain a finer blend, two times extrusion was carried out. In this case, a ''network'' structure with two-continuous phases was observed for the blends with two compositions of PC/ABS, being 80/20 and 70/30. It is found that the blends with these two compositions just have maximum values on the curves of notched Izod impact strength, flexural modulus and flexural strength vs. composition, respectively. This was never observed in previous publications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The excimer fluorescence of a triblock copolymer, styrene-butadiene-styrene (SBS) containing 48 wt% polystyrene was used to investigate its miscibility with poly(vinyl methyl ether) (PVME). The excimer-to-monomer emission intensity ratio I(M)/I(E) can be used as a sensitive probe to determine the miscibility level in SBS/PVME blends: I(M)/I(E) is a function of PVME concentration, and reaches a maximum when the blend contains 60% PVME. The cloud point curve determined by light scattering shows a pseudo upper critical solution temperature diagram, which can be attributed to the effect of PB segments in SBS. The thermally induced phase separation of SBS/PVME blends can be observed by measuring I(M)/I(E), and the phase dissolution process was followed by measuring I(M)/I(E) at different times.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(styrene-acrylic acid)-lanthanide (Ln.PSAA) and poly(ethylene-acrylic acid)-neodymium (NdPEAA) complexes have been prepared and characterized. The infrared and X-ray photoelectron spectra indicate that the lanthanide complexes possess the bidentate carboxylate structure Ln-O-C(R)-O (see structure B in text). The catalytic behavior of the complexes has been described. The catalytic activities of Nd.PSAA and Nd.PEAA are much greater than that of the corresponding low molecular weight catalyst for butadiene polymerization. The activities of various individual lanthanide elements are quite different from one another. Neodymium shows the highest activity. Europium, samarium and the heavy elements exhibit very low or no activities. The cis-1,4 content of the polybutadiene obtained is not affected by different lanthanide elements in the series. The complex with the intermediate content of the functional group has a higher activity than the others. The polymer-supported lanthanide complexes having different constitutions have different catalytic activities. When the molar ratio of lanthanide to the functional group is ca. 0.2, the activity of the complex is in the optimum state. The activity is influenced by the dispersion of the lanthanide metal immobilized on the polymer chain. Catalytic activity can be improved by adding other metals to the catalyst system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Studies using transmission electron microscopy, differential scanning calorimetry, and X-ray diffraction showed correlations between the crystallization behavior of the polydimethylsiloxane (PDMS) block and the morphology of the block copolymer poly (butadiene-b-dimethylsiloxane) (PB-PDMS). When the PDMS component existed as spheres dispersed in a PB matrix, the crystallization rate of the PDMS block was lower than when the PDMS phase existed in rod or cylinder form.