986 resultados para Glass ionomer cement


Relevância:

100.00% 100.00%

Publicador:

Resumo:

A retrospective evaluation of glass ionomer cement (GIC) in middle ear surgery with emphasis on short- and long-term safety was conducted at the tertiary referral center. GIC was applied between 1995 and 2006 in 444 patients in otologic surgery. Technical aspects, safety, benefits and complications due to GIC were analysed until 2011 (follow-up 5-16 years; mean 10 years). GIC was applied in stapes surgery (228 primary, 92 revisions), cochlear implants (108) and implantable hearing aids (7), ossiculoplasty (7), for coverage of opened mastoid air cells towards the external ear canal (1) and inner ear fistula closure (1). GIC turned out to be very handy in stapes surgery for optimal prosthesis fixation at the incus (260) and on the malleus handle (60) without complications. Results suggest that GIC may diminish the danger of incus necrosis in primary stapedotomy. In cochlear implants and implantable hearing aids, GIC was used for casing alone (74), casing and electrode fixation (27) and electrode alone fixation (14). Inflammatory reactions were observed in five cases (4.3 %), mostly after trauma. Broken cement fragments appeared to promote foreign body rejection. In seven cases an incudo-stapedial gap was repaired with GIC with excellent hearing gain; in three cases (43 %) revision surgery was needed due to cement breakage. In one case, GIC was applied for a watertight coverage of opened mastoid cells, and in the other for fistula closure of the lateral semi-circular canal over cartilage, covered with bone pathé; follow-up was uneventful. Targeted use of GIC in middle ear surgery rarely poses problems. GIC cannot be used in neuro-otosurgery in contact with cerebrospinal fluid because of possible aluminium encephalopathy.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Water uptake and water loss have been studied in a commercial resin-modified glass-ionomer cement, Fuji II LC, under a variety of conditions. Uptake was generally non-Fickian, but affected by temperature. At room temperature, the equilibrium water uptake values varied from 2.47 to 2.78% whereas at low temperature (12 degrees C), it varied from 0.85 to 1.18%. Cure time affected uptake values significantly. Water uptake was much lower than in conventional glass-ionomer restorative cements exposed to water vapor. Loss of water under desiccating conditions was found to be Fickian for the first 5 h loss at both 22 and 12 degrees C. Diffusion coefficients were between 0.45 and 0.76 x 10( -7) cm(2)/s, with low temperature diffusion coefficients slightly greater than those at room temperature. Plotting water loss as percentage versus s(-(1/2)) allowed activation energies to be determined from the Arrhenius equation and these were found to be 65.6, 79.8, and 7.7 kJ/mol respectively for 30, 20, and 10 s cure times. The overall conclusion is that the main advantage of incorporating HEMA into resin-modified-glass-ionomers is to alter water loss behavior. Rate of water loss and total amount lost are both reduced. Hence, resin-modified glass-ionomers are less sensitive to water loss than conventional glass-ionomers.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The role of aluminum in glass-ionomers and resin-modified glass-ionomers for dentistry is reviewed. Aluminum is included in the glass component of these materials in the form of Al(2)O(3) to confer basicity on the glass and enable the glass to take part in the acid-base setting reactions. Results of studies of these reactions by FTIR and magic-angle spinning (MAS)-NMR spectroscopy are reported and the role of aluminum is discussed in detail. Aluminum has been shown to be present in the glasses in predominantly 4-coordination, as well as 5- and 6-coordination, and during setting a proportion of this is converted to 6-coordinate species within the matrix of the cement. Despite this, mature cements may contain detectable amounts of both 4- and 5-coordinate aluminum. Aluminum has been found to be leached from glass-ionomer cements, with greater amounts being released under acidic conditions. It may be associated with fluoride, with which it is known to complex strongly. Aluminum that enters the body via the gastro-intestinal tract is mainly excreted, and only about 1% ingested aluminum crosses the gut wall. Calculation shows that, if a glass-ionomer filling dissolved completely over 5 years, it would add only an extra 0.5% of the recommended maximum intake of aluminum to an adult patient. This leads to the conclusion that the release of aluminum from either type of glass-ionomer cement in the mouth poses a negligible health hazard.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This study evaluated the surface microhardness of four glass ionomer cements and a composite resin (Fuji IX, Ketac Molar, Vidrion R, Vitromolar and Z 250). Ten specimens of each glass ionomer cement with 8.0 mm diameter and 5.0 mm high dimensions were made and Vicker's microhardness measurements were taken at 1 day and 1 week after initial setting reaction. The results were analyzed using Student's T test and Tukey test (p < 0.05) and demonstrated that the values of microhardness increased after 1 week, with the exception of Fuji IX. Resin composite Z250 presented the greatest values for microhardness.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

To evaluate the cytotoxic effects of five glass-ionomer cements (GICs) on an odontoblast cell line (MDPC-23), disks of every material were prepared and divided into Group 1: Vitrebond, Group 2: Vitremer, Group 3: Fuji IILC, Group 4: Fuji IX GP, Group 5: Ketac-Molar, Group 6: Z-100 (positive control). In Group 7, phosphate-buffered saline solution (negative control) was applied on filter paper. After placing the samples in the bottom of wells, the cells (30,000 cells/cm(2)) were plated and incubated for 72 h. The cell number was counted, the cell morphology was assessed by scanning electron microscopy and the cell metabolism was evaluated using methyltetrazolium assay. The statistical analysis of Kruskal-Wallis was used to determine if the scores obtained for the cell metabolism and number of cells were different at the 95% confidence level. In groups 1, 2, 3, 4, 5, and 6 the materials decreased the cell number by 74.5% 75.5%, 45.5%, 29.5%, 32.5%, and 88.5%, respectively. In groups 1, 2, 3, 4, and 5, the experimental GICs reduced the cell metabolism by 79%, 84%, 54%, 40%, and 42.5%, respectively. Despite the fact that all experimental materials were cytotoxic to the MDPC-23 cells, the GICs were the least cytotoxic. on the other hand, the RMGICs caused the highest cytophatic effects. (C) 2003 Elsevier B.V. Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objectives. To evaluate the effects of current resin-modified glass-ionomer cements (RMGICs) applied on culture of cells or implanted into subcutaneous tissue of rats.Methods. Experiment 1 - Thirty round-shaped samples of every RMGICs: Rely X Luting Cement (RL), Vitremer (VM), and Vitrebond (VB) were placed into wells with 1.1 mL of culture medium (DMEM), and incubated for 24,48 or 72 h. The extracts from every sample were applied on the MDPC-23 cells. Fresh DMEM was used as control group. The MTT assay was carried out for mitochondrial respiration. Experiment 2 - Fifty-four polyethylene tubes filled with the experimental materials were implanted into the dorsal subcutaneous tissue of rats. At 7, 30, and 90 days the animals were killed and the biopsies were processed for histological evaluation.Results. Experiment 1 - Both time of elution and material significantly influenced cell respiratory activity. in general, the extracts obtained at 24 h were less cytotoxic than 48 and 72 h incubation. The cytotoxic effect of VM and RL were not statistically different (P < 0.05) for the 24-hour period. VB showed the highest cytotoxic effect. Experiment 2 - All RMGICs elicited at 7 days a moderate to intense inflammatory reaction which decreased over time. However, connective healing occurred for most of samples at 90-day evaluation.Significance. Glass-ionomer cements may cause noticeable inflammatory response when in direct contact to connective tissue. The toxic effects of this kind of soluble material depend on the amount of components released in the aqueous environment. (C) 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objective: The aim of this in vitro study was to analyze the effect of glass-ionomer cement as a liner on the dentin/resin adhesive interface of lateral walls of occlusal restorations after thermocycling.Materials and Methods: Occlusal cavities were prepared in 60 human molars, divided into six groups: no liner (1 and 4); glass-ionomer cement (GIC, Ketac Molar Easymix, 3M ESPE) (2 and 5); and resin-modified glass-ionomer cement (RMGIC, Vitrebond, 3M ESPE) (3 and 6). Resin composite (Filtek Z250, 3M ESPE) was placed after application of an adhesive system (Adper Single Bond 2, 3M ESPE) that was mixed with a fluorescent reagent (Rhodamine B) to allow confocal microscopy analysis. Specimens of groups 4, 5 and 6 were thermocycled (5 degrees C-55 degrees C) with a dwell time of 30 seconds for 5000 cycles. After this period, teeth were sectioned in approximately 0.8-mm slices. One slice of each tooth was randomly selected for confocal microscopy analysis. The other slices were sectioned into 0.8 nun x 0.8 mm beams, which were submitted to microtensile testing (MPa). Data were analyzed using two-way ANOVA and Tukey test (p < 0.05).Results: There was no detectedstatistical difference on bond strength among groups (alpha < 0.05). Confocal microscopy analysis showed a higher mean gap size in group 4(12.5 mu m) and a higher percentage of marginal gaps in the thermocycled groups. The RNIGIC liner groups showed the lowest percentage of marginal gaps.Conclusions: Lining with RMGIC resulted in less gap formation at the dentin/resin adhesive interface after artificial aging. RMGIC or GIC liners did not alter the microtensile bond strength of adhesive system/resin composite to dentin on the lateral walls of Class I restorations.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This study aimed to evaluate the influence of fluoride-containing mouthrinse solutions (Fluorgard and Oral B) on the superficial microhardness of two resin-modified glass ionomer cements (Vitremer and Fuji II LC). Fifteen discs-shaped specimens of each glass ionomer cement (0 10 mm; 2 mm thick) were prepared, thereby forming two groups. After 24-hour storage in artificial saliva, the microhardness was measure and the data were recorded. Next, each group was divided into three subgroups (n = 5), according to the solution to be immersed in. Control specimens were kept in artificial saliva along the whole experiment. The test specimens were kept in mouthrinse solution for 30 days. Vickers surface microhardness was analyzed at predetermined evaluation periods: 24 h, 48 h, 7, 14, 21 and 30 days after specimens' preparation. Data were subjected to three-way ANOVA and to Tukey test (p < 0.05). A better behavior of Fuji II LC was observed and Fluorgard affected most the characteristics of the tested materials. It may be concluded that fluoride-containing solutions influenced the tested characteristics of materials, mainly of Vitremer.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objective: A restorative material for Class III cavities must, besides being functional, be esthetically satisfactory, providing good working conditions and several shade and color options. A clinical evaluation was initiated to compare the suitability of resin composite and glass-ionomer cement materials for such restorations.Method and materials: Forty-two Class III conservative cavities, esthetically important because of facial extensions, were selected. Resin composite restorations were placed in 21 cavities, and the remaining 21 were restored with glass-ionomer cement. The following characteristics were studied: color or-esthetics, anatomic shape, surface texture, staining, marginal infiltration, dental plaque retention, and occurrence of fracture. After 24 months, the restorations were evaluated.Results: the only statistically significant difference between the resin composite and glass-ionomer cement restorations in the experimental period involved color or esthetics.Conclusion: Resin composites and glass-ionomer materials provide excellent functional and esthetic results in Class III cavities when properly indicated.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The object of the study was to compare two commercial root canal sealers: Ketac-Endo (a glass ionomer cement) and Fill Canal (a zinc oxide-eugenol cement). A total of 34 root canals from dog premolars with vital pulps were used. After instrumentation, the root canals were sealed with Ketac-Endo and Fill Canal cements using gutta-percha and a lateral condensation technique. After 270 days the animals were sacrificed with an anesthetic overdose and the maxillae and mandibles were removed and fixed in formalin for 48 h. After routine histological processing the sections were stained with hematoxylin-eosin and Mallory trichrome stains. Microscopic analysis revealed that Ketac-Endo cement presented better results than Fill Canal cement.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The purpose of this study was to observe the quality of seal of the glass ionomer cement, Ketac-Endo, after treatment of the root canal wall. The root canals of 140 extracted human teeth were prepared biomechanically. The root canals were treated with either EDTA or received an intracanal dressing of calcium hydroxide or camphorated paramonochlorphenol. The root canals were filled by the lateral condensation technique with gutta-percha points and the sealer Ketac-Endo, or zinc oxide-eugenol cement or Sealapex. The teeth were placed into a 2% methylene blue dye solution inside a flask, which was attached to a vacuum pump. Leakage was measured linearly. Sealapex exhibited significantly less leakage than Ketac-Endo or zinc oxide-eugenol cement (P<0.01). The use of EDTA and intermediary dressings reduced significantly (P<0.01) the leakage observed with the zinc oxide-eugenol sealer and Ketac-Endo.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: To evaluate the surface roughness and staining of a glass ionomer cement when subjected to different finishing procedures. Materials and Methods: Sixty-four discs of Chem-Fil II glass ionomer cement were submitted to staining test with methylene blue by spectrophotometry and roughness test by profilometry. Four groups were evaluated: Mylar matrix (control), Sof-Lex discs, Enhance points, and diamond bur. Results: Staining and roughness test, analyzed by ANOVA and Tukey's test, showed that the best surface was obtained when the material cured in contact with the Mylar matrix strip or when treated with Sof-Lex discs. The poorest results were obtained after using the diamond bur.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This study evaluated the antibacterial activity of the glass-ionomer cements Vitrebond (3M ESPE), Ketac Molar (3M ESPE) and Fuji IX (GC America) against S mutans, S sobrinus, L acidophilus and A viscosus, using the agar diffusion test. Inocula were obtained by the seed of indicators cultures in BHI broth incubated at 37°C for 24 hours. Base layers containing 15 mL of BHI agar and 300 μL of each bacteria suspension were prepared in Petri dishes. Six wells measuring 4 mm in diameter were made in each plate and completely filled with one of the testing materials. A 0.2% chlorhexidine solution applied in round filter papers was used as control. Tests were performed 12 times for each material and bacteria strain. After incubation of the plates at 37°C for 24 hours, the zones of bacterial growth inhibition around the wells were measured. Overall, the results showed the following sequence of antibacterial activity: Vitrebond (despite the activation mode) > 0.2% chlorhexidine > Ketac Molar > Fuji IX, according to Kruskal-Wallis and Mann-Whitney statistical tests. This study confirmed significant antibacterial activity for two conventional glass-ionomers and one resin-modified glass-ionomer material. The resin-modified glass-ionomer cement Vitrebond, regardless of the activation mode, presented the best antibacterial activity against S mutans and S sobrinus. The antibacterial activity against A viscosus for Vitrebond was similar to 0.2% chlorhexidine, while light activation reduced its antibacterial activity against L acidophilus. ©Operative Dentistry, 2005.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The purpose of this study was to evaluate the surface roughness of four conventional chemically cured glass ionomer cements (Fuji IX, Ketac Molar, Vidrion R and Vitromolar) commonly used in atraumatic restorative treatment (ART) immediately after material preparation. Twenty specimens of each glass ionomer cement were fabricated and surface roughness was measured after material setting. The specimens were further examined under scanning electron microscopy. Data were analyzed statistically by Kruskal-Wallis test and Mann-Whitney test at 5% significance level. Two-by-two comparisons showed statistically significant difference (p<0.05) between all materials, except for Ketac Molar and Vidrion R, which had statically similar results (p>0.05). Regarding their results of surface roughness, the materials can be presented in a crescent order, as follows: Ketac Molar < Vidrion R < Fuji IX < Vitromolar. In conclusion, from the tested glass ionomer cements, Fuji IX, Ketac Molar and Vidrion R presented acceptable surface roughness after setting reaction while Vitromolar showed remarkably higher surface roughness.