52 resultados para Luminescence spectroscopy

em Repositório Institucional UNESP - Universidade Estadual Paulista "Julio de Mesquita Filho"


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Hybrid Eu3+-doped silica-poliethyleneoxide (PEO) nanocomposites with covalent bonds between the inorganic (siloxane) and organic (PEO) phases have been obtained by sol-gel process. These materials are transparent, flexible and present high Eu3+ luminescence output. Their luminescence properties, local environment around europium ions and structure have been investigated as a function of europium content. EXAFS measurements indicate that the increase in Eu-doping induces a decrease in Eu3+ coordination number. An increase in symmetry degree around the metal ion is also observed for increasing Eu3+ concentration, while non radiative decay paths from the D-5(0) excited state become more important. SAXS results suggest the preferential interaction of europium ions with ether-type oxygens of the polymer chains. However, the existence of interactions between the cations and the carbonyl groups from urea bridges located at the siloxane-PEO interface can not be excluded.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Good optical quality Eu3+-doped silica-polyethyleneglycol hybrids were prepared by the sol-gel process. Thermomechanical analysis showed an increase of the glass transition temperature, due to the stiffness of the polymeric network, as the amount of Eu3+ increased. Europium luminescent properties were used to study structural evolution during the sol-gel transition. For lower doping concentrations dried gels present statistical distributions of Eu3+, typical of an amorphous environment, while for higher concentrations a crystalline-like environment of Eu3+ was observed. A broad emission band was observed in the visible part of the electromagnetic spectrum and assigned to the intrinsic emission from the hybrid polymeric network.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Nanocrystallized boehmite gamma-AlOOH center dot nH(2)O had been synthesized by spray-drying (SD) of a solution of aluminium tri-sec-butoxide peptized by nitric acid. The sub-micronic spherical particles obtained had an average diameter of 500 nm and were built of 100 nm or less platelet-like sub-particles. The average crystallite size calculated from XRD was 1.6 nm following the b axis (i.e. one unit cell) and 3-4 nm perpendicular to b. As a result of the nanometric sizes of crystallites, there was a large surface free for water adsorption and it was found to be n = 1.18 +/- 0.24H(2)O per AlOOH. The SD spheres spontaneously dispersed in water at room temperature and formed stable-over months-suspensions with nanometre-size particles (25-85 nm). Luminescent europium-doped nanocrystallized boehmites AlOOH: Eu (Al0.98Eu0.02OOH center dot nH(2)O) were synthesized the same way by SD and demonstrated the same crystallization properties and morphologies as the undoped powders. It is inferred from the Eu3+ luminescence spectroscopy that partly hydrated europium species are immobilized on the boehmite nanocrystals where they are directly bonded to alpha(OH) groups of the AlOOH surface. The europium coordination is schematically written [Eu3+(OH)(alpha)(H2O)(7-alpha/2)]. The europium-doped boehmite from SD spontaneously dispersed in water: the luminescence spectroscopy proves that most of the Eu3+ ions were detached from the NPs during water dispersion. The AlOOH: Eu nanoparticles were modified by the amine acid asparagine (ASN). The modification aimed to render the NPs compatible for further bio-functionalization. After surface modification, the NPs easily dispersed in water; the luminescence spectra after dispersion prove that the Eu3+ ions were held at the boehmite surface.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Transparent, flexible, and luminescent EU3+-doped siloxane-poly(ethylene glycol) (PEG) nanocomposites have been obtained by the sol-gel process. The inorganic (siloxane) and organic PEG phases are usually linked by weak bonds (hydrogen bonds or van der Waals forces), and small-angle X-ray scattering (SAXS) measurements suggest that the structure of these materials consists of fractal siloxane aggregates embedded in the PEG matrix. For low Eu3+ contents, n = 300 and n = 80, the aggregates are small and isolated and their fractal dimensions are 2.1 and 1.7, respectively. These values are close to those expected for gelation mechanisms consisting of reaction-limited cluster-cluster aggregation (RLCCA) and diffusion-limited cluster-cluster aggregation (DLCCA). For high Eu3+ content, SAYS results are consistent with a two-level structure: a primary level of siloxane aggregates and a second level, much larger, formed by the coalescence of the primary ones. The observed increase in the glass transition temperature for increasing Eu3+ content is consistent with the structural model derived from SAXS measurements. Extended X-ray absorption fine structure (EXAFS) and luminescence spectroscopy measurements indicate that under the experimental conditions utilized here Eu3+ ions do not strongly interact with the polymeric phase.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

70.00% 70.00%

Publicador:

Resumo:

We studied the effect of silica surface on luminescence properties of terbium complex by spectroscopy characterization, where microparticles of mesoporous silica type MSU-X was prepared. We used silica with different surface: calcined, washed, functionalized with 3- aminopropyl-triethoxysilane (APTES), and 3-glycidoxypropyl-trimethoxysilane (GPTMS); impregnated with Tb3+-glutamic acid complex. The obtained materials were characterized by scanning electron microscopy, porosity measurements, small-angle X-ray scattering, as structural characterization; Fourier transform infrared and luminescence spectroscopy, as spectroscopy characterization. Finally, we observed that functional groups at the silica surface lead to changes on luminescent properties of the final materials. The observed shift of the absorption and emission bands can be assigned to the effect of the functional groups of mesoporous silica.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This paper provides a review on the latest advances and applications of the luminescence spectroscopy for the development of pharmaceuticals analyses methods, basically based on the photo- and chemiluminescence. The different forms of the drugs determination on pharmaceuticals through the fluorescence and chemiluminescence are discussed. The analyses include the drugs native fluorescence (liquid and solid-phases); the fluorescence from the oxidizing or reducing forms of the drug; the fluorescence from the chemical derivatization and their photochemistry and hydrolysis reactions. The quenching of luminescence and chemiluminescence generation for the pharmaceutical quantification are also shown. Finally, the trends and future perspectives of the luminescence spectroscopy in the field of the pharmaceutical research are discussed.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

These films were obtained by dip coating. Parameters like dislocation velocity; number of deposits, suspension concentration, and number of deposits followed or not by heat treatment between each deposit and calcination temperature were evaluated for establishing the best homogeneity. The obtained films were characterized in terms of their morphology, optical quality and photoluminescence by scanning electron microscopy (SEM), UV-vis absorption spectrophotometry and luminescence spectroscopy, respectively. The morphologic and luminescent characteristics showed dip coating as good laboratory technique for development of thin films for optical applications.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The ZnO luminescent properties are strongly influenced by the preparation method and they are principally related to electronic and crystalline structures. This work reports about the correlation among luminescence properties of ZnO, obtained from zinc hydroxycarbonate, and crystalline lattice defects, microstrain, as function of thermal treatment. The crystallite size increase and the qualitative microstrain, obtained by Williamson-Hall plots, decrease as function of temperature. The evolution of electronic defects is analyzed by luminescence spectroscopy based on energy of the electronic transitions. From excitation spectrum, it is verified two bands around 377 nm and 405 nm attributed to the transitions between valence-conduction bands and valence band to interstitial zinc level, respectively. The emission spectra of sample treated at 600 degreesC shows large band at 670 nm. However, the green emission around 530 nm is observed for samples treated at 900 degreesC. The intensities of excitation and emission bands are associated with the increase of the electronic defects that depend on the strain lattice decrease. The lowest strain lattice results on the best green luminescent properties of zinc oxide. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pure yttrium oxide or mixed with europium oxide (3 at%) were treated in supercritical isopropanolic suspension at 500degreesC for 20 It and filling degree of 50%. Products were supercritically dried and characterized by scanning electron microscopy (SEM), X-ray powder diffraction (XRD), infrared spectroscopy (IR) and luminescence spectroscopy (LS). Particle shape is irregular with an equivalent diameter of ca. 5 mum. Cubic crystalline phase is mainly obtained and hydroxide ion in low concentration is detected by IR vibrational spectrum. Europium in this concentration does not extensively change such observed characteristics from the pure yttrium oxide. Luminescence spectra show that the doped product is a mixture of the two oxides added by oxyhydroxide impurities. Nevertheless, this precursor sample, after being heated at 900degreesC during 1 h, has all characteristics, especially luminescent ones, of the P22 commercial phosphor. (C) 2003 Elsevier B.V. (USA). All rights reserved.