104 resultados para Flexural strength

em QUB Research Portal - Research Directory and Institutional Repository for Queen's University Belfast


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fibre distribution and orientation in a series of round panel specimens of ultra high performance fibre reinforced concrete (UHPFRC) was investigated using electrical resistivity measurements and confirmed by X-ray CT imaging. By pouring specimens in different ways, the orientation of steel fibres was influenced and the sensitivity of the electrical resistivity technique was investigated. The round panels were tested in flexure and the results are discussed in relation to the observed orientation of fibres in the panels. It was found that the fibres tended to align perpendicular to the direction of flow. As a result, panels poured from the centre were significantly stronger than panels poured by other methods because the alignment of fibres led to more fibres bridging the radial cracks formed during mechanical testing.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The ductility of concrete made with commercially available steel and synthetic fibres has been investigated. Flexural stress–deflection relationships have been used to determine: flexural strength, flexural toughness, equivalent flexural strength, and equivalent flexural strength ratio. The flexural toughness of concrete was found to increase considerably when steel and synthetic fibres were used. However, equal dosages of different fibres did not result in specimens with the same flexural toughness. Flexural toughness differences of almost 35 J existed even at the same fibre dosage. This also resulted in considerable differences in the minimum required ground supported slab thickness.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Reinforced concrete (RC) jacketing is a common method for retrofitting existing columns with poor structural performance. It can be applied in two different ways: if the continuity of the jacket is ensured, the axial load of the column can be transferred to the jacket, which will be directly loaded; conversely, if no continuity is provided, the jacket will induce only confinement action. In both cases the strength and ductility evaluation is rather complex, due to the different physical phenomena included, such as confinement, core-jacket composite action, preload and buckling of longitudinal bars.
Although different theoretical studies have been carried out to calculate the confinement effects, a practical approach to evaluate the flexural capacity and ductility is still missing. The calculation of these quantities is often related to the use of commercial software, taking advantage of numerical methods such as fibre method or finite element method.
This paper presents a simplified approach to calculate the flexural strength and ductility of square RC jacketed sections subjected to axial load and bending moment. In particular the proposed approach is based on the calibration of the stress-block parameters including the confinement effect. Equilibrium equations are determined and buckling of longitudinal bars is modelled with a suitable stress-strain law. Moment-curvature curves are derived with simple calculations. Finally, comparisons are made with numerical analyses carried out with the code OpenSees and with experimental data available in the literature, showing good agreement.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Bioresorbable polymers such as polylactide (PIA) and polylactide-co-glycolide (PLGA) have been used successfully as biomaterials in a wide range of medical applications. However, their slow degradation rates and propensity to lose strength before mass have caused problems. A central challenge for the development of these materials is the assurance of consistent and predictable in vivo degradation. Previous work has illustrated the potential to influence polymer degradation using electron beam (e-beam) radiation. The work addressed in this paper investigates further the utilisation of e-beam radiation in order to achieve a more surface specific effect. Variation of e-beam energy was studied as a means to control the effective penetrative depth in poly-L-lactide (PLEA). PLEA samples were exposed to e-beam radiation at individual energies of 0.5 MeV, 0.75 MeV and 1.5 MeV. The near-surface region of the PLEA samples was shown to be affected by e-beam irradiation with induced changes in molecular weight, morphology, flexural strength and degradation profile. Moreover, the depth to which the physical properties of the polymer were affected is dependent on the beam energy used. Computer modelling of the transmission of each e-beam energy level used corresponded well with these findings. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A study undertaken at the University of Liverpool has investigated the potential for using construction and demolition waste (C&DW) derived aggregate in the manufacture of a range of precast concrete products, i.e. building and paving blocks and pavement flags. Phase III, which is reported here, investigated
concrete pavement flags. This was subsequent to studies on building and paving blocks. Recycled demolition aggregate can be used to replace newly quarried limestone aggregate, usually used in coarse (6 mm) and fine (4 mm-to-dust) gradings. The first objective was, as was the case with concrete building
and paving blocks, to replicate the process used by industry in fabricating concrete pavement flags in the laboratory. The ‘‘wet’’ casting technique used by industry for making concrete flags requires a very workable mix so that the concrete flows into the mould before it is compressed. Compression squeezes out water from the top as well as the bottom of the mould. This industrial casting procedure was successfully replicated in the laboratory by using an appropriately modified cube crushing machine and a special mould typical of what is used by industry. The mould could be filled outside of the cube crushing machine and then rolled onto a steel frame and into the machine for it to be compressed. The texture and mechanical properties of the laboratory concrete flags were found to be similar to the factory ones. The experimental work involved two main series of tests, i.e. concrete flags made with concrete- and
masonry-derived aggregate. Investigation of flexural strength was required for concrete paving flags. This is different from building blocks and paving blocks which required compressive and tensile splitting strength respectively. Upper levels of replacement with recycled demolition aggregate were determined
that produced similar flexural strength to paving flags made with newly quarried aggregates, without requiring an increase in the cement content. With up to 60% of the coarse or 40% of the fine fractions replaced with concrete-derived aggregates, the target mean flexural strength of 5.0 N/mm2 was still
achieved at the age of 28 days. There was similar detrimental effect by incorporating the fine masonry-derived aggregate. A replacement level of 70% for coarse was found to be satisfactory and also conservative. However, the fine fraction replacement could only be up to 30% and even reduced to 15% when used for mixes where 60% of the coarse fraction was also masonry-derived aggregate.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This paper describes a series of four-point bending tests that were conducted, under service loads and to failure, on unreinforced, reinforced and post-tensioned glulam timber beams, where the reinforcing tendon used was 12 mm diameter toughened steel bar. The research was designed to evaluate the benefits offered by including an active reinforcement in contrast to the passive reinforcement typically used within timber strengthening works, in addition to establishing the effect that bonding the reinforcing tendon has on the materials performance.

The laboratory investigations established that the flexural strength and stiffness increased for both the reinforced and post-tensioned timbers compared to the unreinforced beams. The flexural strength of the reinforced timber increased by 29.4%, while the stiffness increased by 28.1%. Timber that was post-tensioned with an unbonded steel tendon showed a flexural strength increase of 17.6% and an increase in stiffness of 8.1%. Post-tensioned beams with a bonded steel tendon showed increases in flexural strength and stiffness of 40.1% and 30% respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Improvements in the structural performance of glulam timber beams by the inclusion of reinforcing materials can increase both the service performance and ultimate capacity. This paper describes a series of four-point bending tests conducted, under service loads and to failure, on unreinforced, reinforced and post-tensioned glulam timber beams, where the reinforcing tendon used is 12 mm dia. basalt fibre-reinforced polymer. The research is designed to evaluate the benefits offered by including an active reinforcement in contrast to the passive reinforcement typically used within timber strengthening works, in addition to establishing the effect that bonding the reinforcing tendon has on the material's performance. Further experimental tests have also been developed to investigate the long-term implications of this research, with emphasis placed upon creep and loss of post-tensioning; however, this is ongoing and is not presented in this paper. The laboratory investigations establish that the flexural strength and stiffness increase for both the unbonded and bonded post-tensioned timbers compared to the unreinforced and reinforced beams. Timber that is post-tensioned with an unbonded basalt fibre-reinforced polymer tendon shows a flexural strength increase of 2ṡ8% and an increase in stiffness of 8ṡ7%. Post-tensioned beams with a bonded basalt fibre-reinforced polymer tendon show increases in flexural strength and stiffness of 15ṡ4% and 11ṡ5% respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Improvements in the structural performance of glulam timber beams by the inclusion of reinforcing materials can increase both the service performance and ultimate capacity. In recent years research focusing on the addition of fibre reinforced polymers (FRP) to strengthen members has yielded positive results. However, the FRP material is still relatively expensive and its full potential in combination with structural timber has not been realised. This paper describes a series of four-point bending tests that were conducted, under service loads and to failure, on unreinforced, reinforced and post-tensioned glulam timber beams, where the reinforcing tendon used was 12mm diameter basalt fibre reinforced polymer (BFRP). The research was designed to evaluate the benefits offered by including an active reinforcement in contrast to the passive reinforcement typically used within timber strengthening works, in addition to establishing the affect that bonding the reinforcing tendon has on the material’s performance. Further experimental tests have been developed to investigate the long-term implications of this research, with emphasis placed upon creep and loss of post-tensioning.
The laboratory investigations established that the flexural strength and stiffness increased for both the unbonded and bonded post-tensioned timbers compared to the unreinforced beams. Timber that was post-tensioned with an unbonded BFRP tendon showed a flexural strength increase of 2.8% and an increase in stiffness of 8.7%. Post-tensioned beams with a bonded BFRP tendon showed increases in flexural strength and stiffness of 16.6% and 11.5% respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Many timber structures may require strengthening due to either decay and aging or an increase of load. This paper presents an experimental study in which eleven timber beams were tested, including three unstrengthened reference beams and eight beams strengthened with NSM CFRP bars. The test parameters include the position of NSM (tensile face or the bottom of the sides), the number of CFRP bars (1 or 2), and additional anchorage of NSM CFRP bars (steel wire U anchors or CFRP U strips). The test results show that the ultimate flexural strength of the timber beams were increased by 14%∼85% with an average of 47% due to NSM CFRP bar strengthening. Their deflection corresponding to the peak load was increased by 33% in average.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Reinforced concrete (RC) jacketing is a common method to retrofit existing columns with poor structural performance. It can be applied in two different ways: if the continuity of the jacket is ensured, the axial load of the column can be transferred to the jacket, which will be directly loaded; conversely, if no continuity is provided, the jacket induces only confinement action. In both cases the strength and ductility evaluation is rather complex, due to the different physical phenomena included, such as confinement, composite action core-jacket, preload, buckling of longitudinal bars.
Although different theoretical studies have been carried out to calculate the confinement effects, a practical approach to evaluate the flexural capacity and ductility is still missing. The calculation of these quantities is often related to the use of commercial computer programs, taking advantage of numerical methods such as fiber method or finite element method.
This paper presents a simplified approach to calculate the flexural strength and ductility of square RC jacketed sections subjected to axial load and bending moment. In particular the proposed approach is based on the calibration of the stress-block parameters including the confinement effect. Equilibrium equations are determined and buckling of longitudinal bars is modeled with a suitable stress-strain law. Moment-curvature curves are derived with simple calculations. Finally, comparisons are made with numerical analyses carried out with the code OpenSees and with experimental data available in the literature, showing good agreement.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The building sector requires the worldwide production of 4 billion tonnes of cement annually, consuming more than 40% of global energy and accounting for about 8% of the total CO2 emissions. The SUS-CON project aimed at integrating waste materials in the production cycle of concrete, for both ready-mixed and pre-cast applications, resulting in an innovative light-weight, ecocompatible and cost-effective construction material, made by all-waste materials and characterized by enhanced thermal insulation performance and low embodied energy and CO2. Alkali activated “cementless” binders, which have recently emerged as eco-friendly construction materials, were used in conjunction with lightweight recycled aggregates to produce sustainable concrete for a range of applications. This paper presents some results from the development of a concrete made with a geopolymeric binder (alkali activated fly ash) and aggregate from recycled mixed plastic. Mix optimisation was achieved through an extensive investigation on production parameters for binder and aggregate. The mix recipe was developed for achieving the required fresh and hardened properties. The optimised mix gave compressive strength of about 7 MPa, flexural strength of about 1.3 MPa and a thermal conductivity of 0.34 W/mK. Fresh and hardened properties were deemed suitable for the industrial production of precast products. Precast panels were designed and produced for the construction of demonstration buildings. Mock-ups of about 2.5 x 2.5 x 2.5 m were built at a demo park in Spain both with SUS-CON and Portland cement concrete, monitoring internal and external temperatures. Field results indicate that the SUS-CON mock-ups have better insulation. During the warmest period of the day, the measured temperature in the SUS-CON mock-ups was lower.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In this work NiO/3mol% Y2O3-ZrO2 (3YSZ) and NiO/8mol% Y2O3-ZrO2 (8YSZ) hollow fibers were prepared by phase-inversion. The effect of different kinds of YSZ (3YSZ and 8YSZ) on the porosity, electrical conductivity, shrinkage and flexural strength of the hollow fibers were systematically evaluated. When compared with Ni-8YSZ the porosity and shrinkage of Ni-3YSZ hollow fibers increases while the electrical conductivity decreases, while at the same time also exhibiting enhanced flexural strength. Single cells with Ni-3YSZ and Ni-8YSZ hollow fibers as the supported anode were successfully fabricated showing maximum power densities of 0.53 and 0.67Wcm-2 at 800°C, respectively. Furthermore, in order to improve the cell performance, a Ni-8YSZ anode functional layer was added between the electrolyte and Ni-YSZ hollow fiber. Here enhanced peak power densities of 0.79 and 0.73Wcm-2 were achieved at 800°C for single cells with Ni-3YSZ and Ni-8YSZ hollow fibers, respectively.