The present investigation addresse the influence of laser welding process-ing parameters used for joining dis-similar metals (ferritic to austenitic steel), on the induced residual stress field. Welding was performed on a Nd:YAG laser DY033 (3300 W) in a continuous wave (CW), keyhole mode. The base metals (BM) employed in this study are AISI 1010 carbon steel (CS) and AISI 304L austenitic stainless steel (SS). Pairs of dissimilar plates of 200 mm x 45 mm x 3 mm were butt joined by laser welding. Different sets of parameters were used to engineer the base metals apportionment at joint formation, namely distinct dilution rates. Residual strain scanning, carried out by neutron diffraction was used to assess the joints. Through-thickness residual stress maps were determined for the laser welded samples of dis-similar steels using high spatial reso-lution. As a result, an appropriate set of processing parameters, able to mi-nimize the local tensile residual stress associated to the welding process, was found.

Formato

application/pdf

Identificador

http://oa.upm.es/29034/

Idioma(s)

eng

Publicador

E.T.S.I. Caminos, Canales y Puertos (UPM)

Relação

http://oa.upm.es/29034/1/INVE_MEM_2013_167127.pdf

http://www.publieve.com/detnumero.php?rev=5&num=88

Direitos

http://creativecommons.org/licenses/by-nc-nd/3.0/es/

info:eu-repo/semantics/restrictedAccess

Fonte

Soldadura y tecnologías de unión, ISSN 1130-0280, 2013-12, Vol. 24, No. 135

Palavras-Chave #Materiales
Tipo

info:eu-repo/semantics/article

Artículo

PeerReviewed