Resumo

Objective: This study aimed at evaluating the degree of conversion (DC) of four composite resins, being one nanofilled and 3 microhybrid resins, photo-activated with second- and third-generation light-emitting diodes (LEDs). Material and methods: Filtek (TM) Z350 nanofilled composite resins and Amelogen (R) Plus, Vit-l-escence (TM) and Opallis microhybrid resins were photo-activated with two second-generation LEDs (Radii-cal and Elipar Free Light (TM) 2) and one third-generation LED (Ultra-Lume LED 5) by continuous light mode, and a quartz halogen-tungsten bulb (QHT, control). After 24 h of storage, the samples were pulverized into fine powder and 5 mg of each material were mixed with 100 mg of potassium bromide (KBr). After homogenization, they were pressed, which resulted in a pellet that was evaluated using an infrared spectromer (Nexus 470, Thermo Nicolet) equipped with TGS detector using diffuse reflectance (32 scans, resolution of 4 cm(-1)) coupled to a computer. The percentage of unreacted carbon-carbon double bonds (% C=C) was determined from the ratio of absorbance intensities of aliphatic C=C (peak at 1637 cm-1) against internal standard before and after curing of the specimen: aromatic C-C (peak at 1610 cm-1). Results: The ANOVA showed a significant effect on the interaction between the light-curing units (LCUs) and the composite resins (p<0.001). The Tukey's test showed that the nanofilled resin (Filtek (TM) Z350) and Opallis when photo-activated by the halogen lamp (QTH) had the lowest DC compared with the other microhybrid composite resins. The DC of the nanofilled resin (Filtek (TM) Z350) was also lower using LEDs. The highest degrees of conversion were obtained using the third-generation LED and one of second-generation LEDs (Elipar Free Light (TM) 2). Conclusions: The nanofilled resin showed the lowest DC, and the Vit-l-escence (TM) microhybrid composite resin showed the highest DC. Among the LCUs, it was not possible to establish an order, even though the second-generation LED Radii-cal provided the lowest DC.

Identificador

JOURNAL OF APPLIED ORAL SCIENCE, BAURU-SP, v. 20, n. 2, pp. 212-217, MAR-APR, 2012

1678-7757

http://www.producao.usp.br/handle/BDPI/36214

10.1590/S1678-77572012000200015 

http://dx.doi.org/10.1590/S1678-77572012000200015 

Idioma(s)

eng

Publicador

UNIV SAO PAULO FAC ODONTOLOGIA BAURU

BAURU-SP

Relação

JOURNAL OF APPLIED ORAL SCIENCE

Direitos

openAccess

Copyright UNIV SAO PAULO FAC ODONTOLOGIA BAURU

Palavras-Chave #COMPOSITE RESINS #FOURIER TRANSFORM INFRARED SPECTROSCOPY #NANOTECHNOLOGY #LIGHT #DENTAL RESINS #INFRARED-SPECTROSCOPY #LIGHT-INTENSITY #CURING UNITS #POLYMERIZATION #CURE #TEMPERATURE #CONTRACTION #HALOGEN #STRESS #DENTISTRY, ORAL SURGERY & MEDICINE
Tipo

article

original article

publishedVersion