Strength of 3Y-TZP and feldspathic porcelain subjected to different cooling methods


Autoria(s): Almeida-júnior, Antonio Alves De; Longhini, Diogo; Galvão, Beatriz Regalado; Santos, Claudinei Dos; Adabo, Gelson Luis
Contribuinte(s)

Universidade Estadual Paulista (UNESP)

Data(s)

02/02/2015

02/02/2015

01/04/2014

Resumo

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

AIM: To investigate the effect of the cooling rate on flexural strength of monolayer and bilayer porcelain/zirconia (Y-TZP) bars. METHODS: Forty-five specimens were made for each design group: (PM) monolithic specimens of veneer porcelain Vita VM9 (Vita, Germany); (ZM) monolithic specimens of zirconia (ZiHP; ProtMat, Brazil); (PB) bilayer specimens zirconia/porcelain with porcelain on lower surface; and (ZB) bilayer specimens porcelain/zirconia with zirconia on lower surface. Each group was cooled by three different methods after porcelain sintering: slow specimens were cooled inside the turned-off furnace; normal specimens were removed from the furnace and cooled in air at room temperature; and fast specimens were removed from the furnace at 910°C and cooled by compressed air for 10 s. Specimens were polished and flexural strength was measured in water at 37 °C (n=15). Maximum load at fracture was recorded, and equations for simple (monolayer) and composite (bilayer) structures were used to calculate the flexural strength. RESULTS were analyzed using one-way ANOVA (p<0.05) and Tukey test separately for each design. RESULTS: The results of one-way ANOVA were statistically significant only for the PB group. The post-hoc Tukey test showed the highest flexural strength for fast cooling and the lowest for slow cooling; the normal cooling was statistically similar to both. CONCLUSIONS: Cooling methods affected only the flexural strength of bilayer specimens with porcelain on low surface (under tension) when the slow cooling method was used.

Formato

124-128

Identificador

http://dx.doi.org/10.1590/1677-3225v13n2a09

Brazilian Journal of Oral Sciences. Faculdade de Odontologia de Piracicaba - UNICAMP, v. 13, n. 2, p. 124-128, 2014.

1677-3225

http://hdl.handle.net/11449/114365

10.1590/1677-3225v13n2a09

S1677-32252014000200124

S1677-32252014000200124.pdf

Idioma(s)

eng

Publicador

Faculdade de Odontologia de Piracicaba - UNICAMP

Relação

Brazilian Journal of Oral Sciences

Direitos

openAccess

Palavras-Chave #dental porcelain #zirconium #material resistance
Tipo

info:eu-repo/semantics/article