Preparation of Y1.84La0.16O3 nanopowders by oxalate co-precipitation method
Data(s) |
2006
|
---|---|
Resumo |
Nanopowder of Y(1.84)mLa(0.16)O(3) was prepared by oxalate co-precipitation method. The powder was characterized by TG-DTA, XRD and TEM. The results show that the precursor is Re-2 (NO3)(2) (C2O4)(2)center dot 2H(2)O (Re=Y, La), and the Y1.84La0.16O3 nanopowders produced by calcining the precursor at 1000 degrees C for 4 h are 20 similar to 40 nm spherical particles and well dispersed. The powders were with high sintering activity and could be fabricated to transparent ceramic without additive at 1450 similar to 1550 degrees C in H-2 atmosphere for 3 hours. The total transmission of the transparent ceramic could reach 80%. |
Identificador | |
Idioma(s) |
英语 |
Fonte |
Tang Zai-Feng;Ding Jun;杨秋红;徐军.,无机化学学报,2006,22(10):1871-1873 |
Palavras-Chave | #光学材料;晶体 #Y(1.84)Lao(0.16)O(3) #nanopowder #oxalate co-precipitation method #transparent ceramic |